C95200
Cast
BRONZES
Copper-Aluminum-Iron and Copper-Aluminum-Iron-Nickel Alloys (Aluminium Bronzes)
true
true
https://api.copper.org/alloys.xhtml/C95200
Elements | |||
---|---|---|---|
Cu(1) | Fe | Al | |
(1) Cu + Sum of Named Elements 99.0% min. |
|||
Min (%) | 86.0 | 2.5 | 8.5 |
Max (%) | 4.0 | 9.5 |
Form | Temper | Temper Code | Tensile Strength (ksi) |
YS-0.5% Ext (ksi) |
Elongation (%) |
Rockwell B scale | Brinell Hardness, 3000 kg load | Shear Strength (ksi) |
Izod (ft-lbs) |
Charpy V-Notch Impact Strength (ft-lbs) |
Charpy Un-Notched Impact Strength | Compressive Strength .001 in. set/in. (ksi) |
Compressive Strength .1 in. set/in. (ksi) |
Creep Strength (0.1% per 10,000 hours) (ksi) |
Fatigue Strength** (ksi) |
Proportional Limit (ksi) |
---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
* Measured at room temperature, 68°F (20°C). ** Fatigue Strength: 100 x 106 cycles, unless indicated as [N] x 106. | ||||||||||||||||
As Centrifugal Cast | As Centrifugal Cast | M02 |
65 Min for Standard 65 Min for Standard |
25 Min for Standard |
20 Min for Standard 20 Min for Standard |
110 Min for Standard |
||||||||||
As Continuous Cast | As Continuous Cast | M07 |
68 Min for Standard 68 Min for Standard |
26 Min for Standard |
20 Min for Standard 20 Min for Standard |
|||||||||||
As Permanent Mold Cast | As Permanent Mold Cast | M05 |
93 Typ |
35 Typ |
38 Typ |
78 Typ |
||||||||||
As Sand Cast | As Sand Cast | M01 |
65 Min for Standard 65 Min for Standard 80 Typ |
25 Min for Standard 27 Typ |
20 Min for Standard 20 Min for Standard 35 Typ |
110 Min for Standard 125 Typ |
40 Typ |
30 Typ | 30 Typ |
20 Typ | 27 Typ | 70 Typ | 7.9 Typ | 22 Typ | 12 Typ |
(1)Field Strength 16000 A/m(200 Oersteds) | |
Melting Point - Liquidus°F | 1913 |
---|---|
Melting Point - Solidus°F | 1907 |
Densitylb/cu in. at 68°F | 0.276 |
Specific Gravity | 7.64 |
Electrical Conductivity% IACS at 68°F | 11 |
Thermal ConductivityBtu/ sq ft/ ft hr/ °F at 68°F | 29.1 |
Coefficient of Thermal Expansion 68-57210 to -6 power per °F (68 – 572°F) | 9 |
Specific Heat CapacityBtu/ lb /°F at 68°F | 0.09 |
Modulus of Elasticity in Tensionksi | 15000 |
Magnetic Permeability | 1.1 (1) |
Poisson's Ratio | 0.31 |
Casting Attribute | Level |
---|---|
Casting Yield | Low |
Drossing | High |
Effect of Section Size | Low |
Fluidity | Medium |
Gassing | Medium |
Patternmakers Shrinkage inches per inch | 4/16 |
Shrinkage in Solidification | High |
Shrinkage During Freezing | High |
Technique | Suitability |
---|---|
Soldering | Good |
Brazing | Good |
Oxyacetylene Welding | Not Recommended |
Gas Shielded Arc Welding | Excellent |
Coated Metal Arc Welding | Good |
Machinability Rating | 20 |
Common Fabrication Processes
No fabrication process properties for this alloy
Treatment | Value* | Time** | ||
---|---|---|---|---|
* Temperature is measured in Fahrenheit. ** Time is measured in minutes. | ||||
Stress Relief | 600 | |||
Solution Treatment | 0 |
Product Category | Product | Reason Category | Reason |
---|---|---|---|
Electrical | Electrical Hardware | Conductivity (Thermal) | Thermal Conductivity |
Electrical Hardware | Corrosion Resistance | Corrosion Resistance (Excellent) | |
Electrical Hardware | Mechanical Properties | High Strength | |
Fasteners | Nuts | Corrosion Resistance | Corrosion Resistance (Excellent) |
Nuts | Machining Properties | Machinability, Good | |
Nuts | Mechanical Properties | High Strength | |
Industrial | Acid Resistant Pumps | Corrosion Resistance | Corrosion Resistance (Excellent) |
Acid Resistant Pumps | Corrosion Resistance | Corrosion Resistance to Acids | |
Acid Resistant Pumps | Corrosion Resistance | Corrosion Resistance to Fresh Water | |
Acid Resistant Pumps | Corrosion Resistance | Corrosion Resistance to Saline Solutions | |
Acid Resistant Pumps | Friction & Wear Properties | Wear Resistance | |
Acid Resistant Pumps | Machining Properties | Machinability, Good | |
Acid Resistant Pumps | Mechanical Properties | High Strength | |
Bearing Liners | Corrosion Resistance | Corrosion Resistance (Excellent) | |
Bearing Liners | Friction & Wear Properties | Wear Resistance | |
Bearing Liners | Mechanical Properties | High Strength | |
Bearings | Corrosion Resistance | Corrosion Resistance (Excellent) | |
Bearings | Friction & Wear Properties | Wear Resistance | |
Bearings | Machining Properties | Machinability, Good | |
Bearings | Mechanical Properties | High Strength | |
Bushings | Corrosion Resistance | Corrosion Resistance (Excellent) | |
Bushings | Friction & Wear Properties | Wear Resistance | |
Bushings | Machining Properties | Machinability, Good | |
Bushings | Mechanical Properties | High Strength | |
Gears | Corrosion Resistance | Corrosion Resistance (Excellent) | |
Gears | Friction & Wear Properties | Wear Resistance | |
Gears | Machining Properties | Machinability, Good | |
Gears | Mechanical Properties | High Strength | |
High Strength Clamps | Corrosion Resistance | Corrosion Resistance | |
High Strength Clamps | Mechanical Properties | High Strength | |
Hot Mill Guides | Conductivity (Thermal) | Thermal Conductivity | |
Hot Mill Guides | Corrosion Resistance | Corrosion Resistance (Excellent) | |
Hot Mill Guides | Friction & Wear Properties | Wear Resistance | |
Hot Mill Guides | Mechanical Properties | High Strength | |
Hot Mill Guides | Mechanical Properties | Retains Strength at Elevated Temperatures | |
Hydrant Parts | Corrosion Resistance | Corrosion Resistance (Excellent) | |
Hydrant Parts | Corrosion Resistance | Corrosion Resistance to Brackish Water | |
Hydrant Parts | Corrosion Resistance | Corrosion Resistance to Fresh Water | |
Hydrant Parts | Friction & Wear Properties | Wear Resistance | |
Hydrant Parts | Machining Properties | Machinability, Good | |
Hydrant Parts | Mechanical Properties | High Strength | |
Large Gear Parts | Corrosion Resistance | Corrosion Resistance (Excellent) | |
Large Gear Parts | Friction & Wear Properties | Wear Resistance | |
Large Gear Parts | Mechanical Properties | High Strength | |
Mild Alkali Applications | Corrosion Resistance | Corrosion Resistance (Excellent) | |
Mild Alkali Applications | Corrosion Resistance | Corrosion Resistance to Acids | |
Mild Alkali Applications | Friction & Wear Properties | Wear Resistance | |
Mild Alkali Applications | Mechanical Properties | High Strength | |
Pickling Equipment | Corrosion Resistance | Corrosion Resistance (Excellent) | |
Pickling Equipment | Corrosion Resistance | Corrosion Resistance to Acids | |
Pickling Equipment | Machining Properties | Machinability, Good | |
Pickling Equipment | Mechanical Properties | High Strength | |
Pickling Tanks | Corrosion Resistance | Corrosion Resistance (Excellent) | |
Pickling Tanks | Corrosion Resistance | Corrosion Resistance to Acids | |
Pickling Tanks | Friction & Wear Properties | Wear Resistance | |
Pickling Tanks | Mechanical Properties | High Strength | |
Plungers | Corrosion Resistance | Corrosion Resistance (Excellent) | |
Plungers | Friction & Wear Properties | Wear Resistance | |
Plungers | Machining Properties | Machinability, Good | |
Plungers | Mechanical Properties | High Strength | |
Pump Parts | Corrosion Resistance | Corrosion Resistance (Excellent) | |
Pump Parts | Corrosion Resistance | Corrosion Resistance to Acids | |
Pump Parts | Corrosion Resistance | Corrosion Resistance to Fresh Water | |
Pump Parts | Corrosion Resistance | Corrosion Resistance to Saline Solutions | |
Pump Parts | Friction & Wear Properties | Wear Resistance | |
Pump Parts | Machining Properties | Machinability, Good | |
Pump Parts | Mechanical Properties | High Strength | |
Pump Rods | Corrosion Resistance | Corrosion Resistance (Excellent) | |
Pump Rods | Friction & Wear Properties | Wear Resistance | |
Pump Rods | Machining Properties | Machinability, Good | |
Pump Rods | Mechanical Properties | High Strength | |
Thrust Pads | Corrosion Resistance | Corrosion Resistance (Excellent) | |
Thrust Pads | Friction & Wear Properties | Wear Resistance | |
Thrust Pads | Mechanical Properties | High Strength | |
Valve Bodies | Corrosion Resistance | Corrosion Resistance (Excellent) | |
Valve Bodies | Friction & Wear Properties | Wear Resistance | |
Valve Bodies | Machining Properties | Machinability, Good | |
Valve Bodies | Mechanical Properties | High Strength | |
Valve Seats | Corrosion Resistance | Corrosion Resistance | |
Valve Seats | Corrosion Resistance | Corrosion Resistance (Excellent) | |
Valve Seats | Friction & Wear Properties | Wear Resistance | |
Valve Seats | Machining Properties | Machinability, Good | |
Valve Seats | Mechanical Properties | High Strength | |
Valves | Corrosion Resistance | Corrosion Resistance (Excellent) | |
Valves | Friction & Wear Properties | Wear Resistance | |
Valves | Machining Properties | Machinability, Good | |
Valves | Mechanical Properties | High Strength | |
Wear Plates | Corrosion Resistance | Corrosion Resistance (Excellent) | |
Wear Plates | Friction & Wear Properties | Wear Resistance | |
Wear Plates | Mechanical Properties | High Strength | |
Welding Jaws | Conductivity (Thermal) | Thermal Conductivity | |
Welding Jaws | Corrosion Resistance | Corrosion Resistance (Excellent) | |
Welding Jaws | Mechanical Properties | High Strength | |
Welding Jaws | Mechanical Properties | Retains Strength at Elevated Temperatures | |
Worm Wheels | Corrosion Resistance | Corrosion Resistance (Excellent) | |
Worm Wheels | Friction & Wear Properties | Wear Resistance | |
Worm Wheels | Machining Properties | Machinability, Good | |
Worm Wheels | Mechanical Properties | High Strength | |
Worms | Corrosion Resistance | Corrosion Resistance (Excellent) | |
Worms | Friction & Wear Properties | Wear Resistance | |
Worms | Machining Properties | Machinability, Good | |
Worms | Mechanical Properties | High Strength | |
Marine | Covers for Marine Hardware | Appearance | Appearance |
Covers for Marine Hardware | Corrosion Resistance | Corrosion Resistance (Excellent) | |
Covers for Marine Hardware | Corrosion Resistance | Corrosion Resistance to Fresh Water | |
Covers for Marine Hardware | Corrosion Resistance | Corrosion Resistance to Salt Water | |
Covers for Marine Hardware | Mechanical Properties | High Strength | |
Marine Engines | Corrosion Resistance | Corrosion Resistance (Excellent) | |
Marine Engines | Corrosion Resistance | Corrosion Resistance to Brackish Water | |
Marine Engines | Corrosion Resistance | Corrosion Resistance to Fresh Water | |
Marine Engines | Friction & Wear Properties | Wear Resistance | |
Marine Engines | Mechanical Properties | Fatigue Properties | |
Marine Engines | Mechanical Properties | High Strength | |
Marine Hardware | Corrosion Resistance | Corrosion Resistance (Excellent) | |
Marine Hardware | Corrosion Resistance | Corrosion Resistance to Fresh Water | |
Marine Hardware | Corrosion Resistance | Corrosion Resistance to Saline Solutions | |
Marine Hardware | Mechanical Properties | High Strength | |
Propellers | Corrosion Resistance | Corrosion Resistance (Excellent) | |
Propellers | Corrosion Resistance | Corrosion Resistance to Brackish Water | |
Propellers | Corrosion Resistance | Corrosion Resistance to Fresh Water | |
Propellers | Friction & Wear Properties | Wear Resistance | |
Propellers | Mechanical Properties | High Strength | |
Propellers | Mechanical Properties | Retains Strength at Elevated Temperatures | |
Ordnance | Gun Mountings | Corrosion Resistance | Corrosion Resistance (Excellent) |
Gun Mountings | Friction & Wear Properties | Wear Resistance | |
Gun Mountings | Mechanical Properties | High Strength | |
Gun Slides | Corrosion Resistance | Corrosion Resistance (Excellent) | |
Gun Slides | Friction & Wear Properties | Wear Resistance | |
Gun Slides | Mechanical Properties | High Strength |
Form | Specific Sub-Form | Application | System | Standard | Description |
---|---|---|---|---|---|
As Centrifugal Cast | Castings | SAE | J461 | WROUGHT AND CAST COPPER ALLOYS | |
Castings | ASME | SB271 | COPPER BASE ALLOY CENTRIFUGAL CASTINGS | ||
Castings | SAE | J462 | CAST COPPER ALLOYS | ||
Castings | ASTM | B271/B271M | COPPER BASE ALLOY CENTRIFUGAL CASTINGS | ||
As Continuous Cast | Castings | SAE | J461 | WROUGHT AND CAST COPPER ALLOYS | |
Castings | ASME | SB505 | COPPER BASE ALLOY CONTINUOUS CASTINGS | ||
Castings | SAE | J462 | CAST COPPER ALLOYS | ||
Castings | ASTM | B505/B505M | COPPER BASE ALLOY CONTINUOUS CASTINGS | ||
As Sand Cast | Castings | ASME | SB148 | ALUMINUM BRONZE SAND CASTINGS | |
Castings | SAE | J462 | CAST COPPER ALLOYS | ||
Castings | ASTM | B763/B763M | COPPER ALLOY SAND CASTINGS FOR VALVE APPLICATIONS | ||
Castings | ASTM | B148 | ALUMINUM BRONZE SAND CASTINGS | ||
Castings | SAE | J461 | WROUGHT AND CAST COPPER ALLOYS | ||
Flanges | ASME | B16.24 | BRONZE PIPE FLANGES AND FLANGED FITTINGS | ||
ASME | SB148 | ALUMINUM BRONZE SAND CASTINGS | |||
ASTM | B148 | ALUMINUM BRONZE SAND CASTINGS | |||
Ingot | |||||
ASTM | B30 | COPPER BASE ALLOYS IN INGOT FORM | |||
Valves |
Corrosion Properties
No Corrosion Properties Available.
DOWNLOAD Standard Designation for Wrought and Cast Alloys [PDF 775KB, includes all alloys]
PLEASE NOTE: This search is best used with Chrome, FFox 3.6+, Safari 2+, Opera 10+ and IE 9+. To report an issue with this page, please contact us.
DISCLAIMER:
The values listed above represent reasonable approximations suitable for general engineering use. Due to commercial variations in compositions and to manufacturing limitations, they should not be used for specification purposes. See applicable ASTM International specification references.
The values listed above represent reasonable approximations suitable for general engineering use. Due to commercial variations in compositions and to manufacturing limitations, they should not be used for specification purposes. See applicable ASTM International specification references.