Loading...
Copper Alloys Search - Basic
Results
C93800
Anti-acid Metal
Cast
BRONZES
Copper-Tin-Lead Alloys (High-Leaded Tin Bronzes)
true
false
https://api.copper.org/alloys.xhtml/C93800
Elements | |||||||||||
---|---|---|---|---|---|---|---|---|---|---|---|
Cu(1) | Pb | Sn | Zn | Fe | P(2) | Ni(3) | Al | S | Sb | Si | |
(1) Cu + Sum of Named Elements 99.0% min. (2) For continuous castings P shall be 1.5% max. (3) Ni value includes Co. |
|||||||||||
Min (%) | 75.0 | 13.0 | 6.3 | ||||||||
Max (%) | 79.0 | 16.0 | 7.5 | 0.8 | 0.15 | 0.05 | 1.0 | 0.005 | 0.08 | 0.8 | 0.005 |
Form | Temper | Temper Code | Tensile Strength (ksi) |
YS-0.5% Ext (ksi) |
Elongation (%) |
Brinell Hardness, 500 kg load | Shear Strength (ksi) |
Izod (ft-lbs) |
Compressive Strength .001 in. set/in. (ksi) |
Compressive Strength .1 in. set/in. (ksi) |
Fatigue Strength** (ksi) |
Proportional Limit (ksi) |
---|---|---|---|---|---|---|---|---|---|---|---|---|
* Measured at room temperature, 68°F (20°C). ** Fatigue Strength: 100 x 106 cycles, unless indicated as [N] x 106. | ||||||||||||
As Centrifugal Cast | As Centrifugal Cast | M02 |
26 Min for Standard 26 Min for Standard 33 Typ |
14 Min for Standard 20 Typ |
12 Min for Standard 12 Min for Standard 12 Typ |
19 Typ | ||||||
As Continuous Cast | As Continuous Cast | M07 |
25 Min for Standard 25 Min for Standard |
16 Min for Standard |
5 Min for Standard 5 Min for Standard |
|||||||
As Sand Cast | As Sand Cast | M01 |
26 Min for Standard 26 Min for Standard 30 Typ |
14 Min for Standard 16 Typ |
12 Min for Standard 12 Min for Standard 18 Typ |
55 Typ |
15 Typ |
5 Typ | 12 Typ | 38 Typ | 10 Typ | 4 Typ |
Melting Point - Liquidus°F | 1730 |
---|---|
Melting Point - Solidus°F | 1570 |
Densitylb/cu in. at 68°F | 0.334 |
Specific Gravity | 9.25 |
Electrical Conductivity% IACS at 68°F | 11 |
Thermal ConductivityBtu/ sq ft/ ft hr/ °F at 68°F | 30.2 |
Coefficient of Thermal Expansion 68-39210 to -6 power per °F (68 – 392°F) | 10.3 |
Specific Heat CapacityBtu/ lb /°F at 68°F | 0.09 |
Modulus of Elasticity in Tensionksi | 10500 |
Incipient Melting°F | 600 |
Magnetic Permeability | 1 |
Casting Attribute | Level |
---|---|
Casting Yield | High |
Drossing | Low |
Effect of Section Size | Low |
Fluidity | High |
Gassing | Medium |
Patternmakers Shrinkage inches per inch | 2/16 |
Shrinkage in Solidification | Low |
Technique | Suitability |
---|---|
Soldering | Good |
Brazing | Poor |
Oxyacetylene Welding | Not Recommended |
Gas Shielded Arc Welding | Not Recommended |
Coated Metal Arc Welding | Not Recommended |
Machinability Rating | 80 |
Common Fabrication Processes
No fabrication process properties for this alloy
Treatment | Value* | Time** | ||
---|---|---|---|---|
* Temperature is measured in Fahrenheit. ** Time is measured in minutes. | ||||
Stress Relief | 500 | |||
Solution Treatment | 0 |
Product Category | Product | Reason Category | Reason |
---|---|---|---|
Industrial | Acid Resisting Applications | Corrosion Resistance | Corrosion Resistance |
Acid Resisting Applications | Corrosion Resistance | Corrosion Resistance to Brackish Water | |
Acid Resisting Applications | Corrosion Resistance | Corrosion Resistance to Many Industrial Chemicals | |
Acid Resisting Applications | Corrosion Resistance | Corrosion Resistance to Numerous Environments | |
Acid Resisting Applications | Friction & Wear Properties | Low Coefficient of Friction | |
Acid Resisting Applications | Friction & Wear Properties | Wear Resistance | |
Backs for Lined Journal Bearings for Locomotives | Corrosion Resistance | Corrosion Resistance | |
Backs for Lined Journal Bearings for Locomotives | Corrosion Resistance | Corrosion Resistance to Numerous Environments | |
Backs for Lined Journal Bearings for Locomotives | Friction & Wear Properties | Low Coefficient of Friction | |
Backs for Lined Journal Bearings for Locomotives | Friction & Wear Properties | Wear Resistance | |
Backs for Lined Journal Bearings for Passenger Cars | Corrosion Resistance | Corrosion Resistance | |
Backs for Lined Journal Bearings for Passenger Cars | Corrosion Resistance | Corrosion Resistance to Numerous Environments | |
Backs for Lined Journal Bearings for Passenger Cars | Friction & Wear Properties | Low Coefficient of Friction | |
Backs for Lined Journal Bearings for Passenger Cars | Friction & Wear Properties | Wear Resistance | |
Bearings | Corrosion Resistance | Corrosion Resistance | |
Bearings | Corrosion Resistance | Corrosion Resistance to Numerous Environments | |
Bearings | Friction & Wear Properties | Anti-Seizing Properties | |
Bearings | Friction & Wear Properties | Low Coefficient of Friction | |
Bearings | Friction & Wear Properties | Wear Resistance | |
Freight Car Bearings | Corrosion Resistance | Corrosion Resistance | |
Freight Car Bearings | Corrosion Resistance | Corrosion Resistance to Numerous Environments | |
Freight Car Bearings | Friction & Wear Properties | Anti-Seizing Properties | |
Freight Car Bearings | Friction & Wear Properties | Low Coefficient of Friction | |
Freight Car Bearings | Friction & Wear Properties | Wear Resistance | |
General Service Bearings for Moderate Pressure | Corrosion Resistance | Corrosion Resistance | |
General Service Bearings for Moderate Pressure | Corrosion Resistance | Corrosion Resistance to Numerous Environments | |
General Service Bearings for Moderate Pressure | Friction & Wear Properties | Anti-Seizing Properties | |
General Service Bearings for Moderate Pressure | Friction & Wear Properties | Low Coefficient of Friction | |
General Service Bearings for Moderate Pressure | Friction & Wear Properties | Wear Resistance | |
Industrial Centrifuges | Corrosion Resistance | Corrosion Resistance | |
Industrial Centrifuges | Corrosion Resistance | Corrosion Resistance to Brackish Water | |
Industrial Centrifuges | Corrosion Resistance | Corrosion Resistance to Many Industrial Chemicals | |
Industrial Centrifuges | Corrosion Resistance | Corrosion Resistance to Numerous Environments | |
Industrial Centrifuges | Friction & Wear Properties | Wear Resistance | |
Low Friction, Moderate Pressure Bushings | Corrosion Resistance | Corrosion Resistance | |
Low Friction, Moderate Pressure Bushings | Corrosion Resistance | Corrosion Resistance to Numerous Environmentss | |
Low Friction, Moderate Pressure Bushings | Friction & Wear Properties | Anti-Seizing Properties | |
Low Friction, Moderate Pressure Bushings | Friction & Wear Properties | Low Coefficient of Friction | |
Low Friction, Moderate Pressure Bushings | Friction & Wear Properties | Wear Resistance | |
Machine Parts | Conductivity (Thermal) | Thermal Conductivity | |
Machine Parts | Corrosion Resistance | Corrosion Resistance | |
Machine Parts | Corrosion Resistance | Corrosion Resistance to Numerous Environments | |
Machine Parts | Friction & Wear Properties | Anti-Seizing Properties | |
Machine Parts | Friction & Wear Properties | Low Coefficient of Friction | |
Machine Parts | Friction & Wear Properties | Wear Resistance | |
Machine Parts | Machining Properties | Excellent Machinability | |
Pump Bodies for Acid Mine Water | Corrosion Resistance | Corrosion Resistance | |
Pump Bodies for Acid Mine Water | Corrosion Resistance | Corrosion Resistance to Brackish Water | |
Pump Bodies for Acid Mine Water | Corrosion Resistance | Corrosion Resistance to Many Industrial Chemicals | |
Pump Bodies for Acid Mine Water | Corrosion Resistance | Corrosion Resistance to Numerous Environments | |
Pump Bodies for Acid Mine Water | Friction & Wear Properties | Wear Resistance | |
Pump Bodies for Acid Mine Water | Machining Properties | Machinability, Good | |
Pump Impellers for Acid Mine Water | Corrosion Resistance | Corrosion Resistance | |
Pump Impellers for Acid Mine Water | Corrosion Resistance | Corrosion Resistance to Brackish Water | |
Pump Impellers for Acid Mine Water | Corrosion Resistance | Corrosion Resistance to Many Industrial Chemicals | |
Pump Impellers for Acid Mine Water | Corrosion Resistance | Corrosion Resistance to Numerous Environments | |
Pump Impellers for Acid Mine Water | Friction & Wear Properties | Wear Resistance | |
Pump Impellers for Acid Mine Water | Machining Properties | Excellent Machinability | |
Pumps | Corrosion Resistance | Corrosion Resistance | |
Pumps | Corrosion Resistance | Corrosion Resistance to Brackish Water | |
Pumps | Corrosion Resistance | Corrosion Resistance to Many Industrial Chemicals | |
Pumps | Corrosion Resistance | Corrosion Resistance to Numerous Environments | |
Pumps | Friction & Wear Properties | Low Coefficient of Friction | |
Pumps | Friction & Wear Properties | Wear Resistance | |
Railroad Applications | Corrosion Resistance | Corrosion Resistance | |
Railroad Applications | Corrosion Resistance | Corrosion Resistance to Numerous Environments | |
Railroad Applications | Friction & Wear Properties | Wear Resistance | |
Railroad Engine Casings | Conductivity (Thermal) | Thermal Conductivity | |
Railroad Engine Casings | Corrosion Resistance | Corrosion Resistance | |
Railroad Engine Casings | Corrosion Resistance | Corrosion Resistance to Numerous Environments | |
Railroad Engine Casings | Friction & Wear Properties | Wear Resistance | |
Railroad Engine Casings | Pressure Tight | Pressure Tight | |
Wearing Material for Rod Bushings | Corrosion Resistance | Corrosion Resistance | |
Wearing Material for Rod Bushings | Corrosion Resistance | Corrosion Resistance to Numerous Environments | |
Wearing Material for Rod Bushings | Friction & Wear Properties | Wear Resistance | |
Wearing Material for Shoes | Corrosion Resistance | Corrosion Resistance | |
Wearing Material for Shoes | Corrosion Resistance | Corrosion Resistance to Numerous Environments | |
Wearing Material for Shoes | Friction & Wear Properties | Wear Resistance | |
Wearing Material for Wedges | Corrosion Resistance | Corrosion Resistance | |
Wearing Material for Wedges | Corrosion Resistance | Corrosion Resistance to Numerous Environments | |
Wearing Material for Wedges | Friction & Wear Properties | Wear Resistance | |
Marine | Large Bearings for Ships | Corrosion Resistance | Corrosion Resistance |
Large Bearings for Ships | Corrosion Resistance | Corrosion Resistance to Brackish Water | |
Large Bearings for Ships | Corrosion Resistance | Corrosion Resistance to Numerous Environments | |
Large Bearings for Ships | Friction & Wear Properties | Anti-Seizing Properties | |
Large Bearings for Ships | Friction & Wear Properties | Low Coefficient of Friction | |
Large Bearings for Ships | Friction & Wear Properties | Wear Resistance | |
Large Bearings for Ships | Machining Properties | Machinability, Good |
Form | Specific Sub-Form | Application | System | Standard | Description |
---|---|---|---|---|---|
As Centrifugal Cast | Castings | SAE | J461 | WROUGHT AND CAST COPPER ALLOYS | |
Castings | ASTM | B271/B271M | COPPER BASE ALLOY CENTRIFUGAL CASTINGS | ||
Castings | SAE | J462 | CAST COPPER ALLOYS | ||
As Continuous Cast | Castings | SAE | J461 | WROUGHT AND CAST COPPER ALLOYS | |
Castings | ASTM | B505/B505M | COPPER BASE ALLOY CONTINUOUS CASTINGS | ||
Castings | SAE | J462 | CAST COPPER ALLOYS | ||
As Permanent Mold Cast | Castings | SAE | J462 | CAST COPPER ALLOYS | |
Castings | SAE | J461 | WROUGHT AND CAST COPPER ALLOYS | ||
As Sand Cast | MILITARY | MIL-C-22229 | COPPER BASE ALLOY CASTINGS (FOR PRESSURE TIGHT APPLICATIONS) | ||
Castings | SAE | J461 | WROUGHT AND CAST COPPER ALLOYS | ||
Castings | ASTM | B763/B763M | COPPER ALLOY SAND CASTINGS FOR VALVE APPLICATIONS | ||
Castings | SAE | J462 | CAST COPPER ALLOYS | ||
Castings | ASTM | B66 | BRONZE CASTINGS IN THE ROUGH FOR LOCOMOTIVE WEARING PARTS | ||
Castings | ASTM | B584 | COPPER ALLOY SAND CASTINGS FOR GENERAL APPLICATIONS | ||
Ingot | ASTM | B30 | COPPER BASE ALLOYS IN INGOT FORM | ||
Corrosion Properties
No Corrosion Properties Available.
DOWNLOAD Standard Designation for Wrought and Cast Alloys [PDF 775KB, includes all alloys]
PLEASE NOTE: This search is best used with Chrome, FFox 3.6+, Safari 2+, Opera 10+ and IE 9+. To report an issue with this page, please contact us.
DISCLAIMER:
The values listed above represent reasonable approximations suitable for general engineering use. Due to commercial variations in compositions and to manufacturing limitations, they should not be used for specification purposes. See applicable ASTM International specification references.
The values listed above represent reasonable approximations suitable for general engineering use. Due to commercial variations in compositions and to manufacturing limitations, they should not be used for specification purposes. See applicable ASTM International specification references.