C89833
Copper Bismuth Alloy
Cast
BRASSES
Copper-Bismuth and Copper-Bismuth-Selenium Alloys
true
true
https://api.copper.org/alloys.xhtml/C89833
Elements | ||||||||||||
---|---|---|---|---|---|---|---|---|---|---|---|---|
Cu(1) | Pb | Sn | Zn | Fe | P | Ni(2) | Al | Bi | S | Sb | Si | |
(1) Cu + Sum of Named Elements 99.3% min. (2) Ni value includes Co. |
||||||||||||
Min (%) | 86.0 | 4.0 | 2.0 | 1.7 | ||||||||
Max (%) | 91.0 | 0.09 | 6.0 | 6.0 | 0.30 | 0.050 | 1.0 | 0.005 | 2.7 | 0.08 | 0.25 | 0.005 |
Form | Temper | Temper Code | Tensile Strength (ksi) |
YS-0.5% Ext (ksi) |
Elongation (%) |
Brinell Hardness, 500 kg load | Izod (ft-lbs) |
---|---|---|---|---|---|---|---|
* Measured at room temperature, 68°F (20°C). | |||||||
As Sand Cast | As Sand Cast | M01 |
37 Typ |
17 Typ |
28 Typ |
60 Typ |
12 Typ |
Melting Point - Liquidus°F | 1877 |
---|---|
Melting Point - Solidus°F | 1454 |
Densitylb/cu in. at 68°F | 0.317 |
Specific Gravity | 8.78 |
Electrical Conductivity% IACS at 68°F | 17.8 |
Thermal ConductivityBtu/ sq ft/ ft hr/ °F at 68°F | 41 |
Coefficient of Thermal Expansion 68-39210 to -6 power per °F (68 – 392°F) | 13 |
Specific Heat CapacityBtu/ lb /°F at 68°F | 0.085 |
Modulus of Elasticity in Tensionksi | 15500 |
Casting Attribute | Level |
---|---|
Casting Yield | High |
Drossing | Low |
Effect of Section Size | Low |
Fluidity | Medium |
Gassing | Medium |
Patternmakers Shrinkage inches per inch | 11/64 |
Shrinkage in Solidification | Low |
Technique | Suitability |
---|---|
Soldering | Excellent |
Brazing | Good |
Oxyacetylene Welding | Not Recommended |
Gas Shielded Arc Welding | Not Recommended |
Coated Metal Arc Welding | Poor |
Machinability Rating | 81 |
Common Fabrication Processes
No fabrication process properties for this alloy
Thermal Properties
No thermal properties for this alloy
Product Category | Product | Reason Category | Reason |
---|---|---|---|
Industrial | Corrosion Resistant, Pressure Tight Castings | Corrosion Resistance | Corrosion Resistance |
Corrosion Resistant, Pressure Tight Castings | Friction & Wear Properties | Wear Resistance | |
Corrosion Resistant, Pressure Tight Castings | Lead-Free | Lead-Free Alternative to Leaded Alloy C83600 | |
Corrosion Resistant, Pressure Tight Castings | Mechanical Properties | Moderate Strength | |
Impellers | Corrosion Resistance | Corrosion Resistance | |
Impellers | Friction & Wear Properties | Wear Resistance | |
Impellers | Lead Free | Lead-Free Alternative to Leaded Alloy C83600 | |
Impellers | Mechanical Properties | Moderate Strength | |
Pumps | Corrosion Resistance | Corrosion Resistance | |
Pumps | Friction & Wear Properties | Wear Resistance | |
Pumps | Lead Free | Lead-Free Alternative to Leaded Alloy C83600 | |
Pumps | Mechanical Properties | Moderate Strength |
Form | Specific Sub-Form | Application | System | Standard | Description |
---|---|---|---|---|---|
As Sand Cast | ASTM | B584 | COPPER ALLOY SAND CASTINGS FOR GENERAL APPLICATIONS | ||
Ingot | ASTM | B30 | COPPER BASE ALLOYS IN INGOT FORM |
Corrosion Properties
No Corrosion Properties Available.
DOWNLOAD Standard Designation for Wrought and Cast Alloys [PDF 775KB, includes all alloys]
PLEASE NOTE: This search is best used with Chrome, FFox 3.6+, Safari 2+, Opera 10+ and IE 9+. To report an issue with this page, please contact us.
DISCLAIMER:
The values listed above represent reasonable approximations suitable for general engineering use. Due to commercial variations in compositions and to manufacturing limitations, they should not be used for specification purposes. See applicable ASTM International specification references.
The values listed above represent reasonable approximations suitable for general engineering use. Due to commercial variations in compositions and to manufacturing limitations, they should not be used for specification purposes. See applicable ASTM International specification references.