Loading...
Copper Alloys Search - Basic
Results
C89320
Cast
BRASSES
Copper-Bismuth and Copper-Bismuth-Selenium Alloys
true
true
https://api.copper.org/alloys.xhtml/C89320
Elements | ||||||||||||
---|---|---|---|---|---|---|---|---|---|---|---|---|
Cu(1) | Pb | Sn | Zn | Fe | P | Ni(2) | Al | Bi | S | Sb | Si | |
(1) Cu + Sum of Named Elements 99.5% min. (2) Ni value includes Co. |
||||||||||||
Min (%) | 87.0 | 5.0 | 4.0 | |||||||||
Max (%) | 91.0 | 0.09 | 7.0 | 1.0 | 0.20 | 0.30 | 1.0 | 0.005 | 6.0 | 0.08 | 0.35 | 0.005 |
Form | Temper | Temper Code | Tensile Strength (ksi) |
YS-0.5% Ext (ksi) |
Elongation (%) |
Brinell Hardness, 500 kg load | Charpy V-Notch Impact Strength (ft-lbs) |
Compressive Strength .01 in. set/in. (ksi) |
---|---|---|---|---|---|---|---|---|
* Measured at room temperature, 68°F (20°C). | ||||||||
As Centrifugal Cast | As Centrifugal Cast | M02 |
35 Min 40 Typ |
18 Min 20 Typ |
15 Min 30 Typ |
70 Typ |
14 Typ |
20 Typ |
As Continuous Cast | As Continuous Cast | M07 |
35 Min for Standard 40 Typ |
18 Min for Standard 20 Typ |
15 Min for Standard 30 Typ |
70 Typ |
14 Typ |
20 Typ |
As Permanent Mold Cast | As Permanent Mold Cast | M05 |
35 Min 40 Typ |
18 Min 20 Typ |
15 Min 30 Typ |
70 Typ |
14 Typ |
20 Typ |
Melting Point - Liquidus°F | 1913 |
---|---|
Melting Point - Solidus°F | 1702 |
Densitylb/cu in. at 68°F | 0.318 |
Specific Gravity | 8.8 |
Electrical Conductivity% IACS at 68°F | 14.7 |
Thermal ConductivityBtu/ sq ft/ ft hr/ °F at 68°F | 32.4 |
Modulus of Elasticity in Tensionksi | 13900 |
Casting Attribute | Level |
---|---|
Casting Yield | High |
Drossing | Low |
Effect of Section Size | Medium |
Fluidity | Medium |
Gassing | Medium |
Shrinkage in Solidification | Low |
Technique | Suitability |
---|---|
Soldering | Excellent |
Brazing | Good |
Oxyacetylene Welding | Not Recommended |
Gas Shielded Arc Welding | Not Recommended |
Coated Metal Arc Welding | Not Recommended |
Machinability Rating | 80 |
Common Fabrication Processes
No fabrication process properties for this alloy
Treatment | Time** | |||
---|---|---|---|---|
** Time is measured in minutes. | ||||
Solution Treatment | 0 |
Product Category | Product | Reason Category | Reason |
---|---|---|---|
Fasteners | Washers | Corrosion Resistance | Corrosion Resistance |
Washers | Lead Free | Lead Free | |
Washers | Machining Properties | Machinability, Good | |
Washers | Mechanical Properties | Moderate Strength | |
Industrial | Backs for Lined Bearings | Corrosion Resistance | Corrosion Resistance |
Backs for Lined Bearings | Friction & Wear Properties | Wear Resistance | |
Backs for Lined Bearings | Lead Free | Lead-Free Alternative to Leaded Alloy | |
Backs for Lined Bearings | Machining Properties | Machinability, Good | |
Cam Bushings for Diesel Engines | Corrosion Resistance | Corrosion Resistance | |
Cam Bushings for Diesel Engines | Friction & Wear Properties | Wear Resistance | |
Cam Bushings for Diesel Engines | Lead Free | Lead-Free Alternative to Leaded Alloy | |
Cam Bushings for Diesel Engines | Machining Properties | Machinability, Good | |
Crankshaft Main Bearings | Corrosion Resistance | Corrosion Resistance | |
Crankshaft Main Bearings | Friction & Wear Properties | Anti-Seizing Properties | |
Crankshaft Main Bearings | Friction & Wear Properties | Low Coefficient of Friction | |
Crankshaft Main Bearings | Friction & Wear Properties | Wear Resistance | |
Crankshaft Main Bearings | Lead Free | Lead-Free Alternative to Leaded Alloy | |
Crankshaft Main Bearings | Machining Properties | Machinability, Good | |
Deep Well Pump Bowl Bushings | Corrosion Resistance | Corrosion Resistance | |
Deep Well Pump Bowl Bushings | Corrosion Resistance | Corrosion Resistance to Numerous Environments | |
Deep Well Pump Bowl Bushings | Friction & Wear Properties | Wear Resistance | |
Deep Well Pump Bowl Bushings | Lead Free | Lead-Free Alternative to Leaded Alloy | |
Deep Well Pump Bowl Bushings | Machining Properties | Machinability, Good | |
Deep Well Pump Line Shaft Bearings | Corrosion Resistance | Corrosion Resistance | |
Deep Well Pump Line Shaft Bearings | Corrosion Resistance | Corrosion Resistance to Many Industrial Chemicals | |
Deep Well Pump Line Shaft Bearings | Corrosion Resistance | Corrosion Resistance to Numerous Environments | |
Deep Well Pump Line Shaft Bearings | Friction & Wear Properties | Wear Resistance | |
Deep Well Pump Line Shaft Bearings | Lead Free | Lead-Free Alternative to Leaded Alloy | |
Deep Well Pump Line Shaft Bearings | Machining Properties | Machinability, Good | |
Electric Motor Bearings | Corrosion Resistance | Corrosion Resistance | |
Electric Motor Bearings | Friction & Wear Properties | Anti-Seizing Properties | |
Electric Motor Bearings | Friction & Wear Properties | Low Coefficient of Friction | |
Electric Motor Bearings | Friction & Wear Properties | Wear Resistance | |
Electric Motor Bearings | Lead Free | Lead-Free Alternative to Leaded Alloy | |
Electric Motor Bearings | Machining Properties | Machinability, Good | |
General Utility Bearings | Corrosion Resistance | Corrosion Resistance | |
General Utility Bearings | Lead Free | Lead Free | |
General Utility Bearings | Machining Properties | Machinability, Good | |
General Utility Bearings | Mechanical Properties | Moderate Strength | |
General Utility Bushings | Corrosion Resistance | Corrosion Resistance | |
General Utility Bushings | Lead Free | Lead Free | |
General Utility Bushings | Machining Properties | Machinability, Good | |
General Utility Bushings | Mechanical Properties | Moderate Strength | |
Guide Bushings for Piston Rods | Corrosion Resistance | Corrosion Resistance | |
Guide Bushings for Piston Rods | Friction & Wear Properties | Anti-Seizing Properties | |
Guide Bushings for Piston Rods | Friction & Wear Properties | Low Coefficient of Friction | |
Guide Bushings for Piston Rods | Friction & Wear Properties | Wear Resistance | |
Guide Bushings for Piston Rods | Lead Free | Lead-Free Alternative to Leaded Alloy | |
Guide Bushings for Piston Rods | Machining Properties | Machinability, Good | |
Guide Bushings for Valves | Corrosion Resistance | Corrosion Resistance | |
Guide Bushings for Valves | Friction & Wear Properties | Anti-Seizing Properties | |
Guide Bushings for Valves | Friction & Wear Properties | Low Coefficient of Friction | |
Guide Bushings for Valves | Friction & Wear Properties | Wear Resistance | |
Guide Bushings for Valves | Lead Free | Lead-Free Alternative to Leaded Alloy | |
Guide Bushings for Valves | Machining Properties | Machinability, Good | |
Hydraulic Gland Seals | Corrosion Resistance | Corrosion Resistance | |
Hydraulic Gland Seals | Friction & Wear Properties | Anti-Seizing Properties | |
Hydraulic Gland Seals | Friction & Wear Properties | Low Coefficient of Friction | |
Hydraulic Gland Seals | Friction & Wear Properties | Wear Resistance | |
Hydraulic Gland Seals | Lead Free | Lead-Free Alternative to Leaded Alloy | |
Hydraulic Gland Seals | Machining Properties | Machinability, Good | |
Main Bearings for Presses | Corrosion Resistance | Corrosion Resistance | |
Main Bearings for Presses | Friction & Wear Properties | Anti-Seizing Properties | |
Main Bearings for Presses | Friction & Wear Properties | Low Coefficient of Friction | |
Main Bearings for Presses | Friction & Wear Properties | Wear Resistance | |
Main Bearings for Presses | Lead Free | Lead-Free Alternative to Leaded Alloy | |
Main Bearings for Presses | Machining Properties | Machinability, Good | |
Piston Pin Bearings | Corrosion Resistance | Corrosion Resistance | |
Piston Pin Bearings | Friction & Wear Properties | Anti-Seizing Properties | |
Piston Pin Bearings | Friction & Wear Properties | Low Coefficient of Friction | |
Piston Pin Bearings | Friction & Wear Properties | Wear Resistance | |
Piston Pin Bearings | Lead-Free | Lead-Free Alternative to Leaded Alloy | |
Piston Pin Bearings | Machining Properties | Machinability, Good | |
Pump Sleeves | Corrosion Resistance | Corrosion Resistance | |
Pump Sleeves | Corrosion Resistance | Corrosion Resistance to Numerous Environments | |
Pump Sleeves | Friction & Wear Properties | Wear Resistance | |
Pump Sleeves | Lead Free | Lead-Free Alternative to Leaded Alloy | |
Rod Bushings | Corrosion Resistance | Corrosion Resistance | |
Rod Bushings | Friction & Wear Properties | Anti-Seizing Properties | |
Rod Bushings | Friction & Wear Properties | Low Coefficient of Friction | |
Rod Bushings | Friction & Wear Properties | Wear Resistance | |
Rod Bushings | Lead Free | Lead-Free Alternative to Leaded Alloy | |
Rod Bushings | Machining Properties | Machinability, Good | |
Rolling Mill Bearings | Corrosion Resistance | Corrosion Resistance | |
Rolling Mill Bearings | Friction & Wear Properties | Anti-Seizing Properties | |
Rolling Mill Bearings | Friction & Wear Properties | Low Coefficient of Friction | |
Rolling Mill Bearings | Friction & Wear Properties | Wear Resistance | |
Rolling Mill Bearings | Lead Free | Lead-Free Alternative to Leaded Alloy | |
Rolling Mill Bearings | Machining Properties | Machinability, Good | |
Seals | Corrosion Resistance | Corrosion Resistance | |
Seals | Friction & Wear Properties | Anti-Seizing Properties | |
Seals | Friction & Wear Properties | Low Coefficient of Friction | |
Seals | Friction & Wear Properties | Wear Resistance | |
Seals | Lead Free | Lead-Free Alternative to Leaded Alloy | |
Seals | Machining Properties | Machinability, Good | |
Sleeve Bushings (for cranes, etc.) | Corrosion Resistance | Corrosion Resistance | |
Sleeve Bushings (for cranes, etc.) | Friction & Wear Properties | Anti-Seizing Properties | |
Sleeve Bushings (for cranes, etc.) | Friction & Wear Properties | Low Coefficient of Friction | |
Sleeve Bushings (for cranes, etc.) | Friction & Wear Properties | Wear Resistance | |
Sleeve Bushings (for cranes, etc.) | Lead Free | Lead-Free Alternative to Leaded Alloy | |
Sleeve Bushings (for cranes, etc.) | Machining Properties | Machinability, Good | |
Spacer Bushings (for Pumps, etc.) | Corrosion Resistance | Corrosion Resistance | |
Spacer Bushings (for Pumps, etc.) | Friction & Wear Properties | Anti-Seizing Properties | |
Spacer Bushings (for Pumps, etc.) | Friction & Wear Properties | Low Coefficient of Friction | |
Spacer Bushings (for Pumps, etc.) | Friction & Wear Properties | Wear Resistance | |
Spacer Bushings (for Pumps, etc.) | Lead Free | Lead-Free Alternative to Leaded Alloy | |
Spacer Bushings (for Pumps, etc.) | Machining Properties | Machinability, Good | |
Wrist Pin Bushings | Corrosion Resistance | Corrosion Resistance | |
Wrist Pin Bushings | Friction & Wear Properties | Anti-Seizing Properties | |
Wrist Pin Bushings | Friction & Wear Properties | Low Coefficient of Friction | |
Wrist Pin Bushings | Friction & Wear Properties | Wear Resistance | |
Wrist Pin Bushings | Lead Free | Lead-Free Alternative to Leaded Alloy | |
Wrist Pin Bushings | Machining Properties | Machinability, Good |
Form | Specific Sub-Form | Application | System | Standard | Description |
---|---|---|---|---|---|
As Continuous Cast | ASTM | B505/B505M | COPPER BASE ALLOY CONTINUOUS CASTINGS | ||
Ingot | ASTM | B30 | COPPER BASE ALLOYS IN INGOT FORM |
Corrosion Properties
No Corrosion Properties Available.
DOWNLOAD Standard Designation for Wrought and Cast Alloys [PDF 775KB, includes all alloys]
PLEASE NOTE: This search is best used with Chrome, FFox 3.6+, Safari 2+, Opera 10+ and IE 9+. To report an issue with this page, please contact us.
DISCLAIMER:
The values listed above represent reasonable approximations suitable for general engineering use. Due to commercial variations in compositions and to manufacturing limitations, they should not be used for specification purposes. See applicable ASTM International specification references.
The values listed above represent reasonable approximations suitable for general engineering use. Due to commercial variations in compositions and to manufacturing limitations, they should not be used for specification purposes. See applicable ASTM International specification references.