Results
C86500
Manganese Bronze
Cast
BRASSES
Manganese Bronze and Leaded Manganese Bronze Alloy (High Strength Yellow Brasses)
true
false
https://api.copper.org/alloys.xhtml/C86500
Elements | ||||||||
---|---|---|---|---|---|---|---|---|
Cu(1,2) | Pb | Sn | Zn | Fe | Ni(3) | Al | Mn | |
(1) In determining Cu min., Cu may be calculated as Cu + Ni. (2) Cu + Sum of Named Elements 99.0% min. (3) Ni value includes Co. |
||||||||
Min (%) | 55.0 | 36.0 | 0.40 | 0.50 | 0.10 | |||
Max (%) | 60.0 | 0.40 | 1.0 | 42.0 | 2.0 | 1.0 | 1.5 | 1.5 |
Form | Temper | Temper Code | Tensile Strength (ksi) |
YS-0.5% Ext (ksi) |
Elongation (%) |
Brinell Hardness, 500 kg load | Brinell Hardness, 3000 kg load | Izod (ft-lbs) |
Charpy V-Notch Impact Strength (ft-lbs) |
Compressive Strength .001 in. set/in. (ksi) |
Compressive Strength .1 in. set/in. (ksi) |
Creep Strength (0.1% per 10,000 hours) (ksi) |
Fatigue Strength** (ksi) |
---|---|---|---|---|---|---|---|---|---|---|---|---|---|
* Measured at room temperature, 68°F (20°C). ** Fatigue Strength: 100 x 106 cycles, unless indicated as [N] x 106. | |||||||||||||
As Centrifugal Cast | As Centrifugal Cast | M02 |
65 Min for Standard 65 Min for Standard |
25 Min for Standard |
20 Min for Standard 20 Min for Standard |
||||||||
As Continuous Cast | As Continuous Cast | M07 |
70 Min for Standard 70 Min for Standard |
25 Min for Standard |
25 Min for Standard 25 Min for Standard |
||||||||
As Sand Cast | As Sand Cast | M01 |
65 Min for Standard 71 Typ |
25 Min for Standard 29 Typ |
20 Min for Standard 30 Typ |
100 Typ |
130 Typ |
32 Typ | 32 Typ |
24 Typ | 79 Typ | 28 Typ | 20 Typ |
(1)Field Strength 16kA/m | |
Melting Point - Liquidus°F | 1616 |
---|---|
Melting Point - Solidus°F | 1583 |
Densitylb/cu in. at 68°F | 0.301 |
Specific Gravity | 8.33 |
Electrical Conductivity% IACS at 68°F | 22 |
Thermal ConductivityBtu/ sq ft/ ft hr/ °F at 68°F | 49.6 |
Coefficient of Thermal Expansion 68-21210 to -6 power per °F (68 – 212°F) | 11.3 |
Specific Heat CapacityBtu/ lb /°F at 68°F | 0.09 |
Modulus of Elasticity in Tensionksi | 15000 |
Magnetic Permeability | 1.09 (1) |
Casting Attribute | Level |
---|---|
Casting Yield | Low |
Drossing | High |
Effect of Section Size | Low |
Fluidity | Medium |
Gassing | Low |
Patternmakers Shrinkage inches per inch | 4/16 |
Shrinkage in Solidification | High |
Technique | Suitability |
---|---|
Soldering | Fair |
Brazing | Fair |
Oxyacetylene Welding | Poor |
Gas Shielded Arc Welding | Poor |
Coated Metal Arc Welding | Poor |
Machinability Rating | 26 |
Common Fabrication Processes
No fabrication process properties for this alloy
Treatment | Value* | Time** | ||
---|---|---|---|---|
* Temperature is measured in Fahrenheit. ** Time is measured in minutes. | ||||
Stress Relief | 500 | |||
Solution Treatment | 0 |
Product Category | Product | Reason Category | Reason |
---|---|---|---|
Automotive | Weld Guns | Conductivity (Thermal) | Thermal Conductivity |
Weld Guns | Corrosion Resistance | Corrosion Resistance | |
Weld Guns | Mechanical Properties | High Strength | |
Builders Hardware | Brackets | Corrosion Resistance | Corrosion Resistance |
Brackets | Mechanical Properties | High Strength | |
Brackets | Mechanical Properties | Toughness | |
Electrical | Electrical Hardware | Conductivity (Electrical) | Electrical Conductivity |
Electrical Hardware | Conductivity (Thermal) | Thermal Conductivity | |
Electrical Hardware | Corrosion Resistance | Corrosion Resistance | |
Electrical Hardware | Mechanical Properties | High Strength | |
Industrial | Compressors | Corrosion Resistance | Corrosion Resistance |
Compressors | Mechanical Properties | High Strength | |
Compressors | Mechanical Properties | Toughness | |
Forming Dies for Wood Pulp Industry | Corrosion Resistance | Corrosion Resistance | |
Forming Dies for Wood Pulp Industry | Friction & Wear Properties | Wear Resistance | |
Forming Dies for Wood Pulp Industry | Mechanical Properties | High Strength | |
Forming Dies for Wood Pulp Industry | Mechanical Properties | Toughness | |
Frames | Machining Characteristics | Excellent Machinability (Free Machining) | |
Frames | Mechanical Properties | High Strength | |
Gears | Corrosion Resistance | Corrosion Resistance | |
Gears | Corrosion Resistance | Corrosion Resistance to Fresh Water | |
Gears | Corrosion Resistance | Corrosion Resistance to Salt Water | |
Gears | Mechanical Properties | High Strength | |
Gears | Mechanical Properties | Toughness | |
Hooks | Corrosion Resistance | Corrosion Resistance | |
Hooks | Mechanical Properties | High Strength | |
Hooks | Mechanical Properties | Toughness | |
Lever Arms | Corrosion Resistance | Corrosion Resistance | |
Lever Arms | Mechanical Properties | High Strength | |
Lever Arms | Mechanical Properties | Toughness | |
Machinery | Conductivity (Thermal) | Thermal Conductivity | |
Machinery | Corrosion Resistance | Corrosion Resistance | |
Machinery | Mechanical Properties | High Strength | |
Machinery | Mechanical Properties | Toughness | |
Machinery Parts (Substituted for Steel and Malleable Iron) | Corrosion Resistance | Corrosion Resistance | |
Machinery Parts (Substituted for Steel and Malleable Iron) | Mechanical Properties | High Strength | |
Machinery Parts (Substituted for Steel and Malleable Iron) | Mechanical Properties | Toughness | |
Machinery Parts requiring High Strength | Conductivity (Thermal) | Thermal Conductivity | |
Machinery Parts requiring High Strength | Corrosion Resistance | Corrosion Resistance | |
Machinery Parts requiring High Strength | Mechanical Properties | High Strength | |
Machinery Parts requiring High Strength | Mechanical Properties | Toughness | |
Pressing Dies for Wood Pulp | Corrosion Resistance | Corrosion Resistance | |
Pressing Dies for Wood Pulp | Friction & Wear Properties | Wear Resistance | |
Pressing Dies for Wood Pulp | Mechanical Properties | High Strength | |
Pressing Dies for Wood Pulp | Mechanical Properties | Toughness | |
Struts | Corrosion Resistance | Corrosion Resistance | |
Struts | Mechanical Properties | High Strength | |
Struts | Mechanical Properties | Toughness | |
Wear Rings for Pressing Dies for Wood Pulp Industry | Corrosion Resistance | Corrosion Resistance | |
Wear Rings for Pressing Dies for Wood Pulp Industry | Friction & Wear Properties | Wear Resistance | |
Wear Rings for Pressing Dies for Wood Pulp Industry | Mechanical Properties | High Strength | |
Wear Rings for Pressing Dies for Wood Pulp Industry | Mechanical Properties | Toughness | |
Marine | Boat Parts | Corrosion Resistance | Corrosion Resistance |
Boat Parts | Corrosion Resistance | Corrosion Resistance to Salt Water | |
Boat Parts | Mechanical Properties | High Strength | |
Clamps | Corrosion Resistance | Corrosion Resistance | |
Clamps | Corrosion Resistance | Corrosion Resistance to Salt Water | |
Clamps | Mechanical Properties | High Strength | |
Clamps | Mechanical Properties | Toughness | |
Covers for Marine Hardware | Appearance | Appearance | |
Covers for Marine Hardware | Corrosion Resistance | Corrosion Resistance | |
Covers for Marine Hardware | Corrosion Resistance | Corrosion Resistance to Salt Water | |
Covers for Marine Hardware | Mechanical Properties | High Strength | |
Propellers for salt and fresh water | Corrosion Resistance | Corrosion Resistance | |
Propellers for salt and fresh water | Corrosion Resistance | Corrosion Resistance to Saline Solutions | |
Propellers for salt and fresh water | Corrosion Resistance | Corrosion Resistance to Salt Water | |
Propellers for salt and fresh water | Mechanical Properties | Ductility | |
Propellers for salt and fresh water | Mechanical Properties | High Strength | |
Rudders | Corrosion Resistance | Corrosion Resistance | |
Rudders | Corrosion Resistance | Corrosion Resistance to Salt Water | |
Rudders | Friction & Wear Properties | Wear Resistance | |
Rudders | Mechanical Properties | High Strength |
Form | Specific Sub-Form | Application | System | Standard | Description |
---|---|---|---|---|---|
As Centrifugal Cast | Castings | ASTM | B271/B271M | COPPER BASE ALLOY CENTRIFUGAL CASTINGS | |
Castings | AMS | 4860 | MANGANESE BRONZE CASTINGS, SAND AND CENTRIFUGAL, AS CAST | ||
Castings | SAE | J462 | CAST COPPER ALLOYS | ||
Castings | SAE | J461 | WROUGHT AND CAST COPPER ALLOYS | ||
As Continuous Cast | Castings | ASTM | B505/B505M | COPPER BASE ALLOY CONTINUOUS CASTINGS | |
As Die Cast | Castings | ASTM | B176 | BRASS DIE CASTINGS | |
As Sand Cast | Castings | AMS | 4860 | MANGANESE BRONZE CASTINGS, SAND AND CENTRIFUGAL, AS CAST | |
Castings | SAE | J462 | CAST COPPER ALLOYS | ||
Castings | ASTM | B584 | COPPER ALLOY SAND CASTINGS FOR GENERAL APPLICATIONS | ||
Castings | SAE | J461 | WROUGHT AND CAST COPPER ALLOYS | ||
Castings | ASTM | B763/B763M | COPPER ALLOY SAND CASTINGS FOR VALVE APPLICATIONS | ||
Ingot | ASTM | B30 | COPPER BASE ALLOYS IN INGOT FORM | ||
FEDERAL | QQ-C-523 | COPPER ALLOY INGOTS: BRASS (YELLOW HIGH STRENGTH) MANGANESE AND MANGANESE-ALUMINUM BRONZE | |||
Valves |
Corrosion Properties
No Corrosion Properties Available.
DOWNLOAD Standard Designation for Wrought and Cast Alloys [PDF 775KB, includes all alloys]
PLEASE NOTE: This search is best used with Chrome, FFox 3.6+, Safari 2+, Opera 10+ and IE 9+. To report an issue with this page, please contact us.
DISCLAIMER:
The values listed above represent reasonable approximations suitable for general engineering use. Due to commercial variations in compositions and to manufacturing limitations, they should not be used for specification purposes. See applicable ASTM International specification references.
The values listed above represent reasonable approximations suitable for general engineering use. Due to commercial variations in compositions and to manufacturing limitations, they should not be used for specification purposes. See applicable ASTM International specification references.