Loading...
Copper Alloys Search - Basic
Results
C23000
Red Brass, 85%
Wrought
BRASSES
Copper-Zinc Alloys (Yellow Brasses)
true
true
https://api.copper.org/alloys.xhtml/C23000
Elements | ||||
---|---|---|---|---|
Cu(1) | Pb | Zn | Fe | |
(1) Cu + Sum of Named Elements 99.8% min. |
||||
Min (%) | 84.0 | |||
Max (%) | 86.0 | 0.05 | Rem | 0.05 |
Product Category | Product | Reason Category | Reason |
---|---|---|---|
Architecture | Etching Parts | Appearance | Appearance |
Etching Parts | Corrosion Resistance | Corrosion Resistance | |
Etching Parts | Mechanical Properties | Moderate Strength | |
Trim | Appearance | Appearance | |
Trim | Corrosion Resistance | Corrosion Resistance | |
Trim | Mechanical Properties | Moderate Strength | |
Weather Strip | Corrosion Resistance | Corrosion Resistance | |
Weather Strip | Corrosion Resistance | Stress Corrosion Cracking Resistance | |
Weather Strip | Mechanical Properties | Retention of Spring Properties | |
Builders Hardware | Kick Plates | Appearance | Appearance |
Kick Plates | Corrosion Resistance | Corrosion Resistance | |
Kick Plates | Corrosion Resistance | Corrosion Resistance to Fresh Water | |
Kick Plates | Corrosion Resistance | Corrosion Resistance to Salt Water | |
Kick Plates | Corrosion Resistance | Dezincification Resistance | |
Kick Plates | Forming Characteristics | Coinability | |
Kick Plates | Forming Characteristics | Formability | |
Kick Plates | Mechanical Properties | High Strength | |
Kick Plates | Plating Characteristics | Plateable | |
Consumer | Badges | Appearance | Appearance |
Badges | Corrosion Resistance | Corrosion Resistance | |
Badges | Corrosion Resistance | Corrosion Resistance to Fresh Water | |
Badges | Corrosion Resistance | Corrosion Resistance to Salt Water | |
Badges | Corrosion Resistance | Dezincification Resistance | |
Badges | Forming Characteristics | Coinability | |
Badges | Forming Characteristics | Formability | |
Badges | Mechanical Properties | High Strength | |
Badges | Plating Characteristics | Platability | |
Coinage | Appearance | Appearance | |
Coinage | Corrosion Resistance | Corrosion Resistance | |
Coinage | Forming Characteristics | Coinability | |
Coinage | Mechanical Properties | Moderate Strength | |
Coinage | Plating Characteristics | Plateable | |
Compacts | Appearance | Appearance | |
Compacts | Appearance | Color | |
Compacts | Corrosion Resistance | Corrosion Resistance | |
Compacts | Forming Characteristics | Formability | |
Compacts | Mechanical Properties | Moderate Strength | |
Costume Jewelry | Appearance | Gold Color | |
Costume Jewelry | Forming Characteristics | Formability | |
Dials | Appearance | Appearance | |
Dials | Appearance | Color | |
Dials | Corrosion Resistance | Corrosion Resistance | |
Dials | Mechanical Properties | Moderate Strength | |
Fire Extinguisher Cases | Corrosion Resistance | Corrosion Resistance | |
Fire Extinguisher Cases | Corrosion Resistance | Stress Corrosion Cracking Resistance | |
Fire Extinguisher Cases | Forming Characteristics | Formability | |
Fire Extinguisher Cases | Mechanical Properties | Moderate Strength | |
Lipstick Containers | Appearance | Appearance | |
Lipstick Containers | Corrosion Resistance | Corrosion Resistance | |
Lipstick Containers | Forming Characteristics | Formability | |
Lipstick Containers | Mechanical Properties | Moderate Strength | |
Medallions | Appearance | Appearance | |
Medallions | Corrosion Resistance | Corrosion Resistance | |
Medallions | Corrosion Resistance | Corrosion Resistance to Sea Water | |
Medallions | Corrosion Resistance | Dezincification Resistance | |
Medallions | Forming Characteristics | Coinability | |
Medallions | Mechanical Properties | High Strength | |
Medallions | Plating Characteristics | Platability | |
Nameplates | Appearance | Appearance | |
Nameplates | Corrosion Resistance | Corrosion Resistance | |
Nameplates | Corrosion Resistance | Corrosion Resistance to Fresh Water | |
Nameplates | Corrosion Resistance | Corrosion Resistance to Salt Water | |
Nameplates | Corrosion Resistance | Dezincification Resistance | |
Nameplates | Forming Characteristics | Coinability | |
Nameplates | Forming Characteristics | Formability | |
Nameplates | Mechanical Properties | High Strength | |
Nameplates | Plating Characteristics | Plateable | |
Plaques | Appearance | Appearance | |
Plaques | Corrosion Resistance | Corrosion Resistance | |
Plaques | Corrosion Resistance | Corrosion Resistance to Salt Water | |
Plaques | Corrosion Resistance | Dezincification Resistance | |
Plaques | Forming Characteristics | Coinability | |
Plaques | Mechanical Properties | High Strength | |
Plaques | Plating Characteristics | Plateable | |
Rouge Boxes | Appearance | Appearance | |
Rouge Boxes | Corrosion Resistance | Corrosion Resistance | |
Rouge Boxes | Forming Characteristics | Formability | |
Rouge Boxes | Mechanical Properties | Moderate Strength | |
Tokens | Appearance | Appearance | |
Tokens | Corrosion Resistance | Corrosion Resistance | |
Tokens | Forming Characteristics | Coinability | |
Tokens | Mechanical Properties | Moderate Strength | |
Tokens | Plating Characteristics | Plateable | |
Zippers | Appearance | Appearance | |
Zippers | Corrosion Resistance | Corrosion Resistance | |
Zippers | Forming Characteristics | Cold Workability | |
Electrical | Conduit | Conductivity (Electrical) | Electrical Conductivity |
Conduit | Conductivity (Thermal) | Thermal Conductivity | |
Conduit | Forming Characteristics | Formability | |
Conduit | Mechanical Properties | Moderate Strength | |
Rotor Bars, AC Motors | Brazing Characteristics | Brazability | |
Rotor Bars, AC Motors | Conductivity (Electrical) | Electrical Resistivity - 37 % IACS | |
Screw Shells | Appearance | Appearance | |
Screw Shells | Corrosion Resistance | Corrosion Resistance | |
Screw Shells | Forming Characteristics | Formability | |
Screw Shells | Mechanical Properties | Moderate Strength | |
Sockets | Corrosion Resistance | Corrosion Resistance | |
Sockets | Forming Characteristics | Formability | |
Sockets | Mechanical Properties | Moderate Strength | |
Fasteners | Eyelets | Appearance | Appearance |
Eyelets | Corrosion Resistance | Corrosion Resistance | |
Eyelets | Forming Characteristics | Formability | |
Eyelets | Mechanical Properties | Moderate Strength | |
Fasteners | Appearance | Appearance | |
Fasteners | Corrosion Resistance | Corrosion Resistance | |
Fasteners | Forming Characteristics | Formability | |
Fasteners | Mechanical Properties | Moderate Strength | |
Industrial | Condenser Tubes | Corrosion Resistance | Corrosion Resistance |
Condenser Tubes | Forming Characteristics | Formability | |
Condenser Tubes | Mechanical Properties | Moderate Strength | |
Condenser Tubes | Welding Characteristics | Weldability | |
Fire Extinguishers | Corrosion Resistance | Corrosion Resistance | |
Fire Extinguishers | Forming Characteristics | Formability | |
Fire Extinguishers | Mechanical Properties | Moderate Strength | |
Flexible Metal Hose | Corrosion Resistance | Corrosion Resistance | |
Flexible Metal Hose | Corrosion Resistance | Stress Corrosion Cracking Resistance | |
Flexible Metal Hose | Forming Characteristics | Formability | |
Flexible Metal Hose | Mechanical Properties | Moderate Strength | |
Heat Exchanger Shells | Conductivity (Thermal) | Thermal Conductivity | |
Heat Exchanger Shells | Corrosion Resistance | Corrosion Resistance | |
Heat Exchanger Shells | Forming Characteristics | Formability | |
Heat Exchanger Shells | Mechanical Properties | Moderate Strength | |
Heat Exchangers | Brazing Characteristics | Brazability | |
Heat Exchangers | Conductivity (Thermal) | Thermal Conductivity | |
Heat Exchangers | Corrosion Resistance | Corrosion Resistance | |
Heat Exchangers | Solderability | Solderability | |
Pickling Crates | Corrosion Resistance | Corrosion Resistance | |
Pickling Crates | Corrosion Resistance | Corrosion Resistance to Acids | |
Pickling Crates | Forming Characteristics | Formability | |
Pickling Crates | Mechanical Properties | Moderate Strength | |
Pump Cylinder Liners | Corrosion Resistance | Corrosion Resistance | |
Pump Cylinder Liners | Forming Characteristics | Formability | |
Pump Cylinder Liners | Mechanical Properties | Moderate to High Strength | |
Radiator Cores | Corrosion Resistance | Corrosion Resistance | |
Radiator Cores | Mechanical Properties | Moderate Strength | |
Tags | Appearance | Appearance | |
Tags | Corrosion Resistance | Corrosion Resistance | |
Tags | Forming Characteristics | Formability | |
Tags | Mechanical Properties | Moderate Strength | |
Tubing for Heat Exchangers | Corrosion Resistance | Corrosion Resistance | |
Tubing for Heat Exchangers | Forming Characteristics | Formability | |
Tubing for Heat Exchangers | Mechanical Properties | Moderate Strength | |
Tubing for Heat Exchangers | Welding Characteristics | Weldability | |
Tubing for Instrumentation | Corrosion Resistance | Corrosion Resistance | |
Tubing for Instrumentation | Forming Characteristics | Formability | |
Tubing for Instrumentation | Mechanical Properties | Moderate Strength | |
Tubing for Instrumentation | Welding Characteristics | Weldability | |
Other | Fire Hose Couplings | Corrosion Resistance | Corrosion Resistance |
Fire Hose Couplings | Mechanical Properties | Moderate to High Strength | |
Plumbing | Fittings | Corrosion Resistance | Corrosion Resistance |
Fittings | Forming Characteristics | Formability | |
Fittings | Mechanical Properties | Moderate Strength | |
J-Bends | Corrosion Resistance | Corrosion Resistance | |
J-Bends | Forming Characteristics | Formability | |
J-Bends | Mechanical Properties | Moderate Strength | |
J-Bends | Solderability | Solderability | |
Pipe | Corrosion Resistance | Corrosion Resistance | |
Pipe | Forming Characteristics | Formability | |
Pipe | Mechanical Properties | Moderate Strength | |
Pipe Nipples | Appearance | Appearance | |
Pipe Nipples | Corrosion Resistance | Corrosion Resistance | |
Pipe Nipples | Mechanical Properties | Moderate to High Strength | |
Pipe Service Lines | Corrosion Resistance | Corrosion Resistance | |
Pipe Service Lines | Forming Characteristics | Formability | |
Pipe Service Lines | Mechanical Properties | Moderate Strength | |
Pipe Service Lines | Solderability | Solderability | |
Pump Lines | Corrosion Resistance | Corrosion Resistance | |
Pump Lines | Forming Characteristics | Formability | |
Pump Lines | Mechanical Properties | Moderate Strength | |
Service Lines | Corrosion Resistance | Corrosion Resistance | |
Service Lines | Forming Characteristics | Formability | |
Service Lines | Mechanical Properties | Moderate Strength | |
Traps | Corrosion Resistance | Corrosion Resistance | |
Traps | Mechanical Properties | Moderate Strength |
DOWNLOAD Standard Designation for Wrought and Cast Alloys [PDF 775KB, includes all alloys]
PLEASE NOTE: This search is best used with Chrome, FFox 3.6+, Safari 2+, Opera 10+ and IE 9+. To report an issue with this page, please contact us.
DISCLAIMER:
The values listed above represent reasonable approximations suitable for general engineering use. Due to commercial variations in compositions and to manufacturing limitations, they should not be used for specification purposes. See applicable ASTM International specification references.
The values listed above represent reasonable approximations suitable for general engineering use. Due to commercial variations in compositions and to manufacturing limitations, they should not be used for specification purposes. See applicable ASTM International specification references.