Fact 10 of 10
World-class golfers like Annika Sorenstam and Nick Price use copper-alloy putters. Sorenstam has used hers to win seven tournaments, according to Bobby Grace, who for the past ten years has made putters out of beryllium copper, brass and tungsten bronze in his plant in St. Pete Beach, Florida.