Fact 4 of 10
The crack in the Liberty Bell is most likely the result of use of scrap bronze at a time when the right casting temperatures couldn't be measured accurately, according to David Verdin, a fifth-generation U.S. bell maker. He suggests that it may also have cooled long enough in its mold before the mold was broken.