Fact 9 of 9
Beginning in the early 16th century, European artists often painted on sheets of copper. Those artists include some of the most famous painters of all time: Leonardo da Vinci, Jan Brueghel, El Greco and Rembrandt. They found that copper provided a smooth, durable surface that held the paint very well and allowed for marvelous effects.