Fact 16 of 17
The standing-seam copper roof at Domino's Farms office park in Ann Arbor, Michigan, is the largest in the USA and may very well be the largest in the world. The roof is 2,897 feet (more than a half-mile) long and 209 feet wide at its widest point. The structure houses the world headquarters of Domino's Pizza among others.