Table 14.2b. Dimensions and Physical Characteristics of Copper Tube: Type L

Nominal or standard size, inchesNominal dimensions, inchesCalculated values (based on nominal dimensions)
Outside diameterInside diameterWall thicknessCross sectional area of bore, sq. inchesWeight of tube only, pounds per linear ft.Weight of tube & water, pounds per linear ft.Volume of tube, per linear ft.
Cu ft.Gal.
14 .375 .315 .030 .078 .126 .160 .00054 .00405
38 .500 .430 .035 .145 .198 .261 .00101 .00753
12 .625 .545 .040 .233 .285 .386 .00162 .0121
58 .750 .666 .042 .348 .362 .506 .00232 .0174
34 .875 .785 .045 .484 .455 .664 .00336 .0251
1 1.125 1.025 .050 .825 .655 1.01 .00573 .0429
114 1.375 1.265 .055 1.26 .884 1.43 .00875 .0655
112 1.625 1.505 .060 1.78 1.14 1.91 .0124 .0925
2 2.125 1.985 .070 3.09 1.75 3.09 .0215 .161
212 2.625 2.465 .080 4.77 2.48 4.54 .0331 .248
3 3.125 2.945 .090 6.81 3.33 6.27 .0473 .354
312 3.625 3.425 .100 9.21 4.29 8.27 .0640 .478
4 4.125 3.905 .110 12.0 5.38 10.1 .0764 .571
5 5.125 4.875 .125 18.7 7.61 15.7 .130 .971
6 6.125 5.845 .140 26.8 10.2 21.8 .186 1.39
8 8.125 7.725 .200 46.9 19.3 39.6 .326 2.44
10 10.125 9.625 .250 72.8 30.1 61.6 .506 3.78
12 12.125 11.565 .280 105 40.4 85.8 .729 5.45