level2b
The fouling of an adjacent non-toxic (vinyl paint) surface in seawater
Figure 20. The influence of 90-10 Cu-Ni on the fouling of an adjacent non-toxic (vinyl paint) surface in seawater during summer fouling season
Photo at 1 week
Photo at 3 weeks
Photo at 7 weeks
Photo at 10 weeks
Photo at 24 weeks