System Design Tables

Table 1 Type K - Copper Tube for Gas Installation - TYPE K

Table 1 Type L - Copper Tube for Gas Installation - TYPE L

Table 1 ACR - Copper Tube for Gas Installation - ACR

Table 1 Type Gas - Copper Tube for Gas Installation - Type Gas

Table 2 - Dimensions and Physical Characteristics of Copper Tube: TYPES K, L, ACR and Gas.

Table 3 - Maximum Capacity* for Copper Tube in a Low Pressure System of Less than 14 inches wc and Pressure Drop of 0.5 inches wc, CFH.**

Table 4 - Maximum Capacity* for Copper Tube in a Low Pressure System of Less than 14 inches wc and Pressure Drop of 1 inch wc, CFH.**

Table 5 - Maximum Capacity* for Copper Tube in an Elevated Pressure System of 2 psig and Pressure Drop of 1.0 psig., CFH.** (Based on atmospheric pressure at sea level)

Table 6 - Maximum Capacity* for Copper Tube in an Elevated Pressure System of 5 psig and Pressure Drop of 3.5 psig, CFH.** (Based on atmospheric pressure at sea level)

Table 7 - Multipliers to be Used with Tables 3 through 6 When Specific Gravity of Gas is Other than 0.60.

LP system - Tables for LP [Liquefied Petroleum] Gas System.

Notes:
* Includes a 20% factor for fittings
** See Table 7.