A4073: Copper-Tube Corrosion in Domestic-Water Systems

Show how to identify and mitigate corrosion of copper tube and fittings in domestic waters. The seven sources of corrosion are discussed: solder-flux-induced pitting attack, hydrogen-sulfide-induced pitting attack, erosion corrosion, cuprosolvency, concentration-cell corrosion, chemistry-related hot- and cold-water pitting. Reprint. BSE Boiler Systems Engineering, June 2005.
(8 pgs.) 1 free (add’l $0.25 ea)
A4015: Copper Tube Handbook
   [6.38 MB]
The most up-to-date guide for specifying and installing copper tube for plumbing, heating, air conditioning and refrigeration. Shows soldering and brazing techniques.
(56 pgs.) 1 free (add’l $1.00 ea)
A4005: Copper Tube Sizing Calculator and Handbook

For design of plumbing systems, fire sprinklers, etc. Slide rule calculates tube diameter, pressure loss, developed length, flow rate, friction loss and flow velocity.
(5 pgs. and a calculator) $5.00
1094: Conditions Contributing to Underground Copper Corrosion

Identifies the possible situations in which copper tube or pipe may be subject to external corrosion underground. Identifies measures to prevent such attack. Reprint, AWWA Journal, August 1984.
(4 pgs.) 1 free (add’l $0.25 ea)
A1070: Corrosion by Potable Waters in Building Systems and Water Treatment to Mitigate Corrosion of Copper Plumbing Systems
[5.18 MB]
Two articles reprinted from Materials Performance, August 1993. The first tells how to avoid pitting attack (cold and hot water), concentration cell, dezincification, erosion and galvanic corrosion. Materials selection, system design and chemical treatment techniques are examined. The second article provides an analysis of water treatment techniques used sucessfully by water utilities or dwelling owners, including the addition of hydrating line, caustic soda, ash or a silicate to the distributed water.
A4018: Guide Specifications on Plumbing
   
Contains standards, references and specifications on copper and copper alloy piping system products and materials. Provides information on installation methods and procedures and minimum recommendations on pipe/tube fittings and joints for specific applications.
(16 pgs, with Microsoft Word© file on a floppy disk) 1 free (add’l $1.00 ea)
A1162: Occurrence and Control of Corrosion in Copper Water Tube Systems

Describes North American and European standards covering tubes, fittings, solders, fluxes and guidelines for assembly of copper tube water systems and the low incidence of corrosion-related failures. Discusses responsibility of water purveyors to provide noncorrosive waters to their customers. Reprint, Proceedings of the 1994 Water Quality Technology Conference, November 1994.
A1095: Overcoming Corrosion Concerns in Copper Tube Systems

Describes proper materials selection, system design and operations, correct workmanship practices and effective water treatment alternatives for mitigating corrosion concerns while satisfying the 1991 Lead-Copper Rule Amendment to the 1974 Safe Drinking Water Act. Reprint, Materials Performance, September 1996.
A1061: Pitting Corrosion of Copper in Cold Potable Water Systems

Examines the influence of water chemistry on cold-water pitting of copper tube. Explains how this low-incidence problem can be mitigated by simply raising the water’s pH and lowering free carbon dioxide to acceptable levels. Reprint, Materials Performance, October 1995.
A1062: Water- and Soil-Side Corrosion of Copper Water Service Lines
[3.50 MB]
Study results of 10- to 70-year underground copper water service lines throughout Billings, Montana, show copper has excellent resistance to indigenous soils and water. Reprint, Materials Performance, March 1995.

How to Order

Download the entire Publication List [PDF - 690Kb]

Download Publication Order Form [PDF - 341Kb]

FAX or MAIL a completed order form to: (888)329-2232 or (203)264-3714 (for foreign orders).

If you need assistance with an order, call CDA at: (212)251-7200.

PLEASE NOTE: Some of the articles featured in the Publications List are now available on our web site in HTML format. They would be marked with this symbol and the publication title would serve as a hyperlink to the listed article.