7044: The Application of Copper-Nickel Alloys in Marine Systems
 
A book of five papers on copper-nickel alloys for marine service covering: properties, corrosion and fouling resistance; seawater piping systems; condenser and heat exchanger applications; usage in desalting plants and equipment; and sheathing of offshore structures and ship hulls. From a series of seminars presented jointly by CDA and the Nickel Development Institute.
(82 pgs.) $5.00
701/5: Brazed Copper-Nickel Piping Systems

Describes, with 10 photographs, 5 drawings and 5 tables, how to braze copper-nickel piping systems, especially for seawater distribution systems where copper-nickel's resistance to biofouling and seawater corrosion is needed.
(6 pgs.) 1 free (add’l $1.00 ea)
A7020: Copper-Nickel Fabrication

Thoroughly reviews the material properties, welding, brazing, fabrication and handling of 90-10 and 70-30 copper-nickels and their applications for pipe systems, condenser service, heat exchangers, boat hulls, sheathing and other structures engineered for marine use.
(28 pgs.) $5.00
708/5: Copper-Nickel Piping for Offshore Platforms
 pdf icon [8.6MB]
C70600 (90-10 Cu-Ni) piping is ideal for offshore platforms on the basis of cost effectiveness, corrosion and biofouling resistance. Includes engineering considerations for installation and fabrication.
(6 pgs.) 1 free (add’l $1.00 ea)
704/4: Copper-Nickel Piping Reduces Costs, Biofouling, Corrosion

Results of a prototype test installation in the Gulf of Mexico show that, although initial costs may sometimes be higher, the life-cycle cost of copper-nickel piping is less and productivity is improved. Reprint, World Oil, November 1984.
(3 pgs.) 1 free (add’l $1.00 ea)
706/5: Copper-Nickel Sheathing Improving Jacket Performance

Describes several prototype applications of 90-10 copper-nickel alloy sheathing of offshore structural members. Includes cost comparisons and design considerations. Reprint, Offshore, November 1985.
(3 pgs.) 1 free (add’l $1.00 ea)
704/5: Design Guide: Copper Alloys Mesh in Marine Aquaculture

Describes prototype fish cages and other aquatic hardware made with copper alloy mesh which resists corrosion and biofouling. Summarizes design data for such installations.
(87 pgs.) $5.00
788/8: Guidelines for the Use of Copper Alloys in Seawater

A thorough presentation of the relative properties and advantages of 18 different copper alloys (including copper itself) in seawater applications. Presents service and laboratory data on resistance to corrosion and biofouling under various environmental conditions. Reprint, Materials Performance, September 1987.
(11 pgs.) 1 free (add’l $1.00 ea)
A1213: Metallic Coatings for Corrosion Control of Marine Structures

Reviews properties of copper-nickel alloys including corrosion behavior and biofouling resistance as affected by composition, water velocity, exposure conditions and methods of attachment to steel. Describes the results of long-term trials of Cu-Ni alloys applied to pilings and ship hulls. Cost benefits are analyzed.
(28 pgs.) 1 free (add’l $1.00 ea)

How to Order

Download the entire Publication List [PDF - 690Kb]

Download Publication Order Form [PDF - 341Kb]

FAX or MAIL a completed order form to: (888)329-2232 or (203)264-3714 (for foreign orders).

If you need assistance with an order, call CDA at: (212)251-7200.

PLEASE NOTE: Some of the articles featured in the Publications List are now available on our web site in HTML format. They would be marked with this symbol and the publication title would serve as a hyperlink to the listed article.