B1 HARD-DRAWN COPPER WIRE
B2 MEDIUM-HARD DRAWN COPPER WIRE
B3 SOFT OR ANNEALED COPPER WIRE
B8 CONCENTRIC-LAY-STRANDED COPPER CONDUCTORS, HARD, MEDIUM-HARD OR SOFT
B9 BRONZE TROLLEY WIRE
B16 FREE-CUTTING BRASS ROD, BAR AND SHAPES FOR USE IN SCREW MACHINES
B19 CARTRIDGE BRASS SHEET, STRIP, PLATE, BAR AND DISKS
B21 NAVAL BRASS ROD, BAR AND SHAPES
B22 BRONZE CASTINGS FOR BRIDGES AND TURNTABLES
B30 COPPER BASE ALLOYS IN INGOT FORM
B33 TINNED SOFT OR ANNEALED COPPER WIRE FOR ELECTRICAL PURPOSES
B36 BRASS PLATE, SHEET, STRIP AND ROLLED BAR
B42 SEAMLESS COPPER PIPE, STANDARD SIZES
B43 SEAMLESS RED BRASS PIPE, STANDARD SIZES
B47 COPPER TROLLEY WIRE
B48 SOFT RECTANGULAR AND SQUARE BARE COPPER WIRE FOR ELECTRICAL CONDUCTORS
B49 HOT-ROLLED COPPER ROD REDRAW FOR ELECTRICAL PURPOSES
B61 STEAM OR VALVE BRONZE CASTINGS
B62 COMPOSITION BRONZE OR OUNCE METAL CASTINGS
B66 BRONZE CASTINGS IN THE ROUGH FOR LOCOMOTIVE WEARING PARTS
B67 CAR AND TENDER JOURNAL BEARINGS, LINED
B68 SEAMLESS COPPER TUBE, BRIGHT ANNEALED
B75 SEAMLESS COPPER TUBE
B88 SEAMLESS COPPER WATER TUBE
B96 COPPER SILICON ALLOY PLATE, SHEET, STRIP AND ROLLED BAR FOR GENERAL PURPOSES AND PRESSURE VESSELS
B98 COPPER-SILICON ALLOY ROD, BAR AND SHAPES
B99 COPPER-SILICON ALLOY WIRE FOR GENERAL PURPOSES
B100 ROLLED COPPER ALLOY BEARING AND EXPANSION PLATES AND SHEETS FOR BRIDGE AND OTHER STRUCTURAL USES
B101 LEAD-COATED COPPER SHEET
B103 PHOSPHOR BRONZE PLATE, SHEET, STRIP AND ROLLED BAR
B105 HARD-DRAWN COPPER ALLOY WIRES FOR ELECTRICAL CONDUCTORS
B111 COPPER AND COPPER ALLOY SEAMLESS CONDENSER TUBES AND FERRULE STOCK
B116 FIGURE 9 DEEP-SECTION GROOVED AND FIGURE 8 COPPER TROLLEY WIRE FOR INDUSTRIAL HAULAGE
B121 LEADED BRASS PLATE, SHEET, STRIP AND ROLLED BAR
B122 COPPER-NICKEL-ZINC ALLOY (NICKEL-SILVER) AND COPPER-NICKEL PLATE, SHEET, STRIP, AND ROLLED BAR
B124 COPPER AND COPPER-ALLOY FORGING ROD, BAR AND SHAPES
B129 CARTRIDGE BRASS CARTRIDGE CASE CUPS
B130 COMMERCIAL BRONZE STRIP FOR BULLET JACKETS
B131 COPPER ALLOY BULLET JACKET CUPS
B133 COPPER ROD, BAR AND SHAPES
B134 BRASS WIRE
B135 SEAMLESS BRASS TUBE
B138 MANGANESE BRONZE ROD, BAR AND SHAPES
B139 PHOSPHOR BRONZE ROD, BAR AND SHAPES
B140 COPPER-ZINC-LEAD (LEADED RED BRASS HARDWARE BRONZE) ROD, BAR AND SHAPES
B148 ALUMINUM BRONZE SAND CASTINGS
B150 ALUMINUM BRONZE ROD, BAR AND SHAPES
B151 COPPER-NICKEL-ZINC ALLOY (NICKEL-SILVER) AND COPPER-NICKEL ROD AND BAR
B152 COPPER SHEET, STRIP, PLATE AND ROLLED BAR
B159 PHOSPHOR BRONZE WIRE
B169 ALUMINUM BRONZE, PLATE, SHEET, STRIP, AND ROLLED BAR
B171 COPPER ALLOY CONDENSER TUBE PLATES
B172 ROPE-LAY-STANDARD CONDUCTORS WITH BUNCH STRANDED MEMBERS
B173 ROPE-LAY-STRANDED CONDUCTORS WITH CONCENTRIC STRANDED MEMBERS
B174 BUNCH-STRANDED CONDUCTORS
B176 BRASS DIE CASTINGS
B187 COPPER BUS BAR, ROD AND SHAPES
B188 SEAMLESS COPPER BUS PIPE AND TUBE
B189 LEAD-COATED AND LEAD ALLOY COATED SOFT COPPER WIRE FOR ELECTRICAL PURPOSES
B194 COPPER BERYLLIUM ALLOY PLATE, SHEET, STRIP, AND ROLLED BAR
B196 COPPER BERYLLIUM ALLOY ROD AND BAR
B197 COPPER BERYLLIUM ALLOY WIRE
B206 COPPER-NICKEL-ZINC ALLOY (NICKEL-SILVER WIRE) AND COPPER-NICKEL ALLOY WIRE
B226 CORED, ANNULAR, CONCENTRIC-LAY-STRANDED COPPER CONDUCTORS
B229 CONCENTRIC-LAY-STRANDED COPPER AND COPPER-CLAD STEEL COMPOSITE CONDUCTORS
B246 TINNED HARD-DRAWN AND MEDIUM HARD-DRAWN COPPER WIRE FOR ELECTRICAL PURPOSES
B271 COPPER BASE ALLOY CENTRIFUGAL CASTINGS
B272 COPPER FLAT PRODUCTS WITH FINISHED (ROLLED OR DRAWN) EDGES (FLAT WIRE AND STRIP)
B280 SEAMLESS COPPER TUBE FOR AIR CONDITIONING AND REFRIGERATION FIELD SERVICE
B283 COPPER AND COPPER ALLOY DIE FORGINGS (HOT PRESSED)
B286 COPPER CONDUCTORS FOR HOOKUP WIRE IN ELECTRONIC EQUIPMENT
B291 COPPER-ZINC-MANGANESE ALLOY (MANGANESE BRASS) SHEET AND STRIP
B298 SILVER-COATED SOFT OR ANNEALED COPPER WIRE
B301 FREE-CUTTING COPPER ROD AND BAR
B302 THREADLESS COPPER PIPE
B306 COPPER DRAINAGE TUBE (DWV)
B315 SEAMLESS COPPER ALLOY PIPE AND TUBE
B355 NICKEL-COATED SOFT OR ANNEALED COPPER WIRE
B359 COPPER AND COPPER-ALLOY SEAMLESS CONDENSER AND HEAT EXCHANGER TUBES WITH INTEGRAL FINS
B360 HARD-DRAWN COPPER CAPILLARY TUBE FOR RESTRICTOR APPLICATIONS
B369 COPPER NICKEL ALLOY CASTINGS
B370 COPPER SHEET AND STRIP FOR BUILDING CONSTRUCTION
B371 COPPER-ZINC-SILICON ALLOY ROD
B372 SEAMLESS COPPER AND COPPER-ALLOY RECTANGULAR WAVEGUIDE TUBE
B395 U-BEND SEAMLESS COPPER AND COPPER ALLOY HEAT EXCHANGER AND CONDENSER TUBES
B411 COPPER-NICKEL-SILICON ALLOY ROD AND BAR
B412 COPPER-NICKEL-SILICON ALLOY WIRE
B422 COPPER-ALUMINUM-SILICON-COBALT ALLOY AND COPPER-NICKEL-ALUMINUM-SILICON ALLOY SHEET AND STRIP
B427 GEAR BRONZE ALLOY CASTINGS
B432 COPPER AND COPPER ALLOY CLAD STEEL PLATE
B441 COPPER-COBALT-BERYLLIUM (UNS NO. C17500) AND COPPER-NICKEL-BERYLLIUM (UNS NO. C17510) ROD AND BAR
B447 WELDED COPPER TUBE
B451 COPPER FOIL, STRIP AND SHEET FOR PRINTED CIRCUITS AND CARRIER TAPES
B453 COPPER-ZINC-LEAD ALLOY (LEADED-BRASS) ROD
B455 COPPER-ZINC-LEAD ALLOY (LEADED-BRASS) EXTRUDED SHAPES
B465 COPPER-IRON ALLOY PLATE, SHEET, STRIP, AND ROLLED BAR
B466 SEAMLESS COPPER-NICKEL PIPE AND TUBE
B467 WELDED COPPER-NICKEL PIPE
B469 SEAMLESS COPPER ALLOY TUBES FOR PRESSURE APPLICATION
B470 BONDED COPPER CONDUCTORS FOR USE IN HOOKUP WIRE FOR ELECTRONIC EQUIPMENT
B492 CAST COPPER-NICKEL SHIP TAILSHAFT SLEEVES
B496 COMPACT ROUND CONCENTRIC-LAY-STRANDED COPPER CONDUCTORS
B505 COPPER BASE ALLOY CONTINUOUS CASTINGS
B506 COPPER CLAD STAINLESS STEEL SHEET AND STRIP FOR BUILDING CONSTRUCTION
B508 COPPER ALLOY STRIP FOR FLEXIBLE METAL HOSE
B534 COPPER-COBALT-BERYLLIUM ALLOY, PLATE, SHEET, STRIP, AND ROLLED BAR
B543 WELDED COPPER AND COPPER ALLOY HEAT EXCHANGER TUBE
B552 SEAMLESS AND WELDED COPPER-NICKEL TUBES FOR WATER DESALTING PLANTS
B569 UNS C26000 BRASS STRIP IN NARROW WIDTHS AND LIGHT GAGE FOR HEAT EXCHANGER TUBING
B570 COPPER-BERYLLIUM ALLOY FORGINGS AND EXTRUSIONS
B584 COPPER ALLOY SAND CASTINGS FOR GENERAL APPLICATIONS
B587 WELDED BRASS TUBE
B591 COPPER-ZINC-TIN ALLOY PLATE, SHEET, STRIP, AND ROLLED BAR
B592 COPPER-ZINC-ALUMINUM-COBALT ALLOY PLATE, SHEET, STRIP, AND ROLLED BAR
B608 WELDED COPPER ALLOY PIPE
B624 HIGH-STRENGTH, HIGH-CONDUCTIVITY COPPER ALLOY WIRE FOR ELECTRONIC APPLICATIONS
B638 COPPER AND COPPER ALLOY SOLAR HEAT ABSORBER PANELS
B640 WELDED COPPER AND COPPER ALLOY TUBE FOR AIR CONDITIONING AND REFRIGERATION SERVICE
B641 SEAMLESS AND WELDED COPPER DISTRIBUTION TUBE (TYPE D)
B643 COPPER-BERYLLIUM ALLOY SEAMLESS TUBE
B687 BRASS, COPPER AND CHROMIUM PLATED PIPE NIPPLES
B694 COPPER, COPPER ALLOY AND COPPER-CLAD STAINLESS STEEL SHEET AND STRIP FOR ELECTRICAL CABLE SHIELDING
B706 SEAMLESS COPPER ALLOY (UNS NO. C69100) PIPE AND TUBE
B716 WELDED COPPER WATER TUBE
B738 FINE-WIRE BUNCH-STRANDED AND ROPE-LAY BUNCH STRANDED COPPER CONDUCTORS FOR USE AS ELECTRICAL CONDUCT
B740 STRIPS, COPPER-NICKEL-TIN SPINODAL ALLOY STRIP
B743 SEAMLESS COPPER TUBE IN COILS
B747 COPPER-ZIRCONIUM ALLOY SHEET AND STRIP
B763 COPPER ALLOY SAND CASTINGS FOR VALVE APPLICATIONS
B768 COPPER-COBALT-BERYLLIUM ALLOY SHEET AND STRIP
F9 ROUND WIRE FOR USE AS GRID SIDE RODS IN ELECTRON TUBES
F68 OXYGEN-FREE COPPER IN WROUGHT FORMS FOR ELECTRON DEVICES
F96 ELECTRONIC GRADE ALLOYS OF COPPER IN WROUGHT FORMS
F467 NONFERROUS NUTS FOR GENERAL USE
F468 NONFERROUS BOLTS, HEX CAP SCREWS, AND STUDS FOR GENERAL USE