print this page

Resources

Loading

Description of AMS Specifications

Specification Description
4500 COPPER SHEET, STRIP AND PLATE, SOFT ANNEALED
4501 COPPER SHEET, STRIP AND PLATE, LIGHT COLD ROLLED
4505 BRASS SHEET, STRIP AND PLATE, ANNEALED
4507 BRASS SHEET, STRIP AND PLATE, HALF-HARD
4508 BRASS SHEET, LAMINATED SURFACE BONDED
4510 PHOSPHOR BRONZE SHEET, STRIP AND PLATE, SPRING TEMPER
4511 COPPER BERYLLINUM ALLOY CASTINGS, SOLUTION AND PRECIPITATION HEAT TREATED
4520 BRONZE STRIP, COLD ROLLED, HALF HARD
4530 COPPER-BERYLLIUM ALLOY SHEET, STRIP, AND PLATE - SOLUTION TREATED
4532 COPPER BERYLLIUM ALOY SHEET AND STRIP, HALF-HARD
4533 COPPER BERYLLINUM ALLOY BARS AND RODS, SOLUTION AND PRECIPITATION HEAT TREATED
4534 COPPER BERYLLIUM ALLOY BARS AND RODS, SOLUTION HEAT TREATED, COLD WORKED AND PRECIPITATION HEAT TREATED
4535 COPPER BERYLLIUM ALLOY MECHANICAL TUBING, SOLUTION AND PRECIPITATION HEAT TREATED
4553 BRASS TUBING, SEAMLESS, SOFT ANNEALED
4554 BRASS TUBING, SEAMLESS, LIGHT ANNEALED
4555 BRASS TUBING SEAMLESS, LIGHT ANNEALED
4558 BRASS TUBING, SEAMLESS DRAWN TEMPER
4590 EXTRUSIONS, NICKEL-ALUMINUM BRONZE, MARTENSITIC, SOLUTION HEAT TREATED AND TEMPERED
4602 COPPER BARS, RODS, AND SHAPES, HARD TEMPER
4610 BRASS BARS AND RODS, FREE CUTTING, HALF-HARD
4611 BRASS BARS AND RODS, NAVAL, HALF-HARD
4612 BRASS BARS AND RODS, NAVAL, HARD TEMPER
4614 BRASS FORGINGS, FREE CUTTING, AS FORGED
4615 SILICON BRONZE ROD AND BAR, HARD TEMPER
4616 SILICON BRONZE BARS, RODS, FORGINGS AND TUBING, STRESS RELIEVED
4619 MANGANESE BRONZE FORGINGS
4625 PHOSPHOR BRONZE BARS, RODS, AND TUBING, HARD TEMPER
4631 ALUMINUM BRONZE RODS, BARS, AND FORGINGS
4635 ALUMINUM BRONZE BARS, RODS, AND FORGINGS, STRESS RELIEVED
4640 ALUMINUM BRONZE BARS, RODS, SHAPES, TUBES, AND FORGINGS
4650 COPPER-BERYLLIUM ALLOY BARS, RODS AND FORGINGS, SOLUTION HEAT TREATED
4651 COPER-BERYLLIUM ALLOY BARS AND RODS, HARD TEMPER
4665 SILICON BRONZE TUBING, SEAMLESS, ANNEALED
4700 COPPER WIRE,BARE, ANNEALED
4701 COPPER WIRE, ANNEALED
4710 BRASS WIRE, TINNED, ANNEALED
4712 BRASS WIRE, ANNEALED
4712 BEARINGS, BABBITT-COATED LEADED BRONZE, STEEL BACK
4713 WIRE, BRASS, EIGHTH-HARD
4720 WIRE, PHOSPHOR BRONZE, COLD DRAWN, SPRING TEMPER
4725 COPPER-BERYLLIUM ALLOY WIRE - SOLUTION HEAT TREATED
4732 COPPER NICKEL ALLOY WIRE AND RIBBON WIRE
4820 BEARINGS, LEADED COPPER, STEEL BACK
4822 BEARINGS, LEADED BRONZE, STEEL BACK
4824 BEARINGS, BABBIT COATED LEADED BRONZE, STEEL BACK
4827 BEARINGS, LEADED BRONZE, STEEL BACK
4842 CASTINGS, LEADED BRONZE, SAND AND CENTRIFUGAL, AS CAST
4845 TIN BRONZE CASTINGS, SAND AND CENTRIFUGAL, AS CAST
4855 LEADED RED BRASS CASTINGS, SAND AND CENTRIFUGAL, AS CAST
4860 MANGANESE BRONZE CASTINGS, SAND AND CENTRIFUGAL, AS CAST
4862 MANGANESE BRONZE CASTINGS, SAND AND CENTRIFUGAL, HIGH STRENGTH, AS CAST
4870 ALUMINUM BRONZE CASTINGS, CENTRIFUGAL AND CHILL, AS CAST
4871 ALUMINUM BRONZE CASTINGS, CENTRIFUGAL AND CHILL, SOLUTION HEAT TREATED AND TEMPERED
4873 ALUMINUM BRONZE CASTINGS, SAND, SOLUTION HEAT TREATED AND TEMPERED
4880 ALUMINUM BRONZE CASTINGS, CENTRIFUGAL AND CONTINUOUS CAST, SOLUTION HEAT TREATED AND TEMPERED
4881 NICKEL-ALUMINUM BRONZE CASTINGS, MARTENSITIC, SAND AND CENTRIFUGAL
4890 COPPER-BERYLLIUM ALLOY CASTINGS, INVESTMENT, HEAT TREATED
7322 SEALING RINGS, CAST TIN BRONZE