New Copper Alloys: Compositions of New Copper Alloys
Copper Applications in Innovative Technology
March 1998
Return To New Copper Alloys
| New Alloy Compositions percent maximum, unless shown as a range or minimum. |
|||
|---|---|---|---|
| C17450 | C17460 | C19710 | |
| Element | Materion Corporation | Materion Corporation | Olin Brass |
| Cu (incl. Ag) | Remainder | Remainder | |
| Cu | Remainder | ||
| Fe | 0.20 | 0.20 | 0.05 - 0.40 |
| Be | 0.15 - 0.50 | 0.15 - 0.50 | |
| Ni | 0.50 - 1.0 | 1.0 - 1.4 | |
| Ni (incl. Co) | 0.10 | ||
| Al | 0.20 | 0.20 | |
| Si | 0.20 | 0.20 | |
| Sn | 0.25 | 0.25 | 0.20 |
| Zr | 0.10 - 0.50 | 0.10 - 0.50 | |
| Zn | 0.20 | ||
| Pb | 0.05 | ||
| P | 0.07 - 0.15 | ||
| Mn | 0.05 | ||
| Mg | 0.03 - 0.06 | ||
| Cu + sum of Named Elements |
99.5 min. | 99.5 min. | 99.5 min. |
| C40810 | C40850 | C40860 | C42520 | |
|---|---|---|---|---|
| Element | Waterbury Rolling Mills -- Tin Brasses | |||
| Cu (incl. Ag) | ||||
| Cu | 94.5 - 96.5 | 94.5 - 96.5 | 94.0 - 96.0 | 88.0 - 91.0 |
| Fe | 0.08 - 0.12 | 0.05 - 0.20 | 0.01 - 0.05 | 0.05 - 0.20 |
| Be | ||||
| Ni | 0.11 - 0.20 | 0.05 - 0.20 | 0.05 - 0.20 | 0.05 - 0.20 |
| Ni (incl. Co) | ||||
| Al | ||||
| Si | ||||
| Sn | 1.8 - 2.2 | 2.6 - 4.0 | 1.7 - 2.3 | 1.5 - 3.0 |
| Zr | ||||
| Zn | Remainder | Remainder | Remainder | Remainder |
| Pb | 0.05 | 0.05 | 0.05 | |
| P | 0.028 - 0.040 | 0.02 - 0.04 | 0.02 - 0.04 | 0.02 - 0.04 |
| Mn | ||||
| Mg | ||||
| Cu + sum of Named Elements |
99.7 min. | 99.7 min. | 99.7 min. | 99.7 min |
| C19025 | C50780 | C51080 | |||
|---|---|---|---|---|---|
| Element | Dowa Mining | Waterbury Rolling Mills -- Phos Bronzes | |||
| Cu | Remainder | Remainder | Remainder | ||
| Sn | 0.7 - 1.1 | 1.7 - 2.3 | 4.8 - 5.8 | ||
| Fe | 0.05 - 0.20 | 0.05 - 0.20 | |||
| Ni | 0.8 - 1.2 | 0.05 - 0.20 | 0.05 - 0.20 | ||
| P | 0.03 - 0.07 | 0.020 - 0.10 | 0.02 - 0.10 | ||
| Pb | 0.05 | 0.05 | |||
| Zn | 0.30 | ||||
| Cu + Sum of Named Elements |
99.7 min. | 99.5 min. | 99.5 min. | ||
Return to New Copper Alloys
Helpful Hints
Innovations was developed to cover technological changes involving copper.
Articles are archived by subject area (see Topics Archives on the left) and by year of publication (see Yearly Archives on the left).
You can also search all of the Copper Development Association's Web site by using Search vox on top right of every page.