How Do They Do That? Wringing Sulfuric Acid out of Sulfur Dioxide Emissions
Copper Applications in Mining & Extraction
November 1997
By BHPOne of the bi-products of the smelting process is the gas sulfur dioxide (S02). Most industrial facilities make a significant effort to reduce the emission of this gas into the air for environmental reasons. For example, at the BHP Copper Metals smelter at San Manuel, Arizona - the largest copper smelter in North America - a sophisticated capture system captures as much as 99 percent of the sulfur dioxide produced in the process.
What is more, the sulfur dioxide that is retained is put through a rigorous process to make a useful product: sulfuric acid, the largest volume chemical used in the world today.
| As little as 1% of the S02is emitted, |
|
The BHP smelter at San Manuel produces 450,000 gallons of sulfuric acid a day, or enough to fill 12,500 rail cars or 52,000 trucks every year.
BHP Copper uses 18 percent of the sulfuric acid it makes for leaching its own oxide ore. Another 40 percent of its sulfuric acid production is sold to other mining companies for their leaching operations.
| On CU is the quarterly publication of BHP Copper, The Broken Hill Proprietary Corp., Ltd. © 1997 BHP Copper |
| ||||
The Latest News
Copper-based Solar Cells:
Good for the Environment, Good for the Consumer
Copper has long been used in solar heating/hot water systems, where it is commonly used in heat exchangers. Now, it promises to become equally valuable in photovoltaic (PV) systems. These systems produce electricity through the action of sunshine on certain semiconductors, including so-called thin-film materials and the currently most promising material: copper indium gallium diselenide or CIGS.
The Presidential Dollars
Golden Collectibles or the Next Coin of the Realm? The U.S. Mint is betting it’s got it right this time. The Mint placed into circulation the first of its new golden dollar coins featuring, for the initial issue, George Washington.
High Strength Copper Steel for Rail Tank Cars to Bridges
This paper shows that the new Copper Steel has advantages over steel presently used in railroad tank cars. The higher strength leads to weight saving; higher impact fracture toughness mitigates against brittle failure particularly at low temperatures. An update of recently completed bridge using the Cu Steel is also provided.
Helpful Hints
Innovations covers technological changes involving copper.
Articles are archived by subject area (see Topics Archives on the left) and by year of publication (see Yearly Archives on the left). You can also search all of the Copper Development Association's Web site by using Search on top right of every page.
If you have articles covering copper technology that you would like to suggest for inclusion here, please send your suggestions to Editors, CDA Innovations.