A Copper Alliance Member
- Applications
- Resources
- Find Suppliers of Copper
- Technical Reference Library
- Publications List
- Automotive
- Building Construction: Architecture
- Building Construction: Fire Sprinklers
- Building Construction: Home Builders' Marketing Materials
- Building Construction: Natural Gas
- Building Construction: Plumbing
- Electrical: Energy Efficiency
- Electrical: General
- Electrical: Power Quality
- Electrical: Telecommunications
- Industrial: Bronze Bearings
- Industrial: Cast Products
- Industrial: General
- Industrial: Machined Rod Products
- Industrial: Mold Alloys
- Properties / Standards
- Seawater
- Soldering / Brazing / Welding
- Special Publications
- Statistics / Directories
- Seminars, Workshops & Training
- Market Data
- Standards
- Properties
- Properties of Wrought and Cast Copper Alloys
- Properties of Copper
- Low Temperature Properties of Copper
- Cryogenic Properties of Copper
- Typical Uses of Copper Alloys
- Copper Compounds
- Microstructures of Copper Alloys
- Corrosion Protection & Resistance
- Fabrication Practices
- Powder Metallurgy
- Metallurgy of Copper-Base Alloys
- Questions?
- Consumers
- Education
- Environment
- Publications
- Newsletters
- Publications List
- Automotive
- Building Construction: Architecture
- Building Construction: Fire Sprinklers
- Building Construction: Home Builders' Marketing Materials
- Building Construction: Natural Gas
- Building Construction: Plumbing
- Electrical: Energy Efficiency
- Electrical: General
- Electrical: Power Quality
- Electrical: Telecommunications
- Industrial: Bronze Bearings
- Industrial: Cast Products
- Industrial: General
- Industrial: Machined Rod Products
- Industrial: Mold Alloys
- Properties / Standards
- Seawater
- Soldering / Brazing / Welding
- Special Publications
- Statistics / Directories
- About CDA
Environment
- Sustainable Energy
- Electric Motors
- Copper Motor Rotor
- Introduction to Premium Efficiency Motors
- NEMA Premium® Motors Mean Big Savings
- A Systems Approach to Calculating Energy Savings
- MotorSlide Calculator™
- High Efficiency Motors & Transformers CD-ROM
- Motor Systems Training
- Creating a Motor Inventory, Repair/Replace Guidelines
- Motor Failure Policies and Purchasing Specifications
- Repair Specifications, and Preventive and Predictive Maintenance
- Mineral Producer Installing 150 Copper-Rotor Motors Rising Energy Costs Drive Upgrades, Rapid Payback Expected
- Copper-Rotor Motors + Variable Frequency Drives Maximize Savings at a Brass Mill
- Copper-Rotor Motors + Variable Frequency Drives Maximize Savings at Water Treatment Plant
- Motor Upgrades Help Cut HVAC Energy Costs
- Kodak Focuses on NEMA Premium®
- Skating Arena Cuts Energy Costs with Premium-Efficiency Motors
- Brass Mill Cuts Costs with NEMA Premium® Motors
- Cummins Engine Company Saves With Energy Efficiency Motors
- Energy Efficiency
- Energy Storage
- Renewables
- Current and Projected Wind and Solar Renewable Electric Generating Capacity in the Domestic Market
- Thermal Modeling of Electrical Conductors
- Copper and Wind Energy
- Driving America to Energy Independence, 30-mph Wind + Plug-In Hybrids = 100 mpg
- 100 Miles of Copper Cable Connects, Protects 4.6-MW Photovoltaic Solar Farm
- Transformers
- High-Efficiency Copper-Wound Transformers Save Energy and Dollars
- Transformer Life Cycle Cost
- High-Efficiency Utility Transformers Mean Lowest Total Owning Cost
- Temperature Rise and Transformer Efficiency
- Introduction to Transformer Losses
- Proper Transformer Sizing & Copper Windings
- Transformer Manufacturer Uses Only Copper
- Energy-Efficient Transformer Yields 156% ROI
- Latest in SE
- Electric Motors
- Mining & Recycling
- Green Properties of Copper
- Copper in Drinking Water
- Copper in the Natural Environment
Melt Copper: Monitoring the Melt Temperature
When melting copper, a lance pyrometer can be used to measure the temperature of the liquid copper. An assembled pyrometer, which is shown in the upper right-hand corner of Figure 9.7.1, uses a type-K thermocouple in a replaceable, graphite-sheathed tip, which is inserted into the liquid copper. Either digital or analog readouts are available. The graphite-sheathed thermocouple will survive numerous insertions into the liquid copper before it will need to be replaced.
Typically lance pyrometers that are inserted into the liquid copper can provide more accurate temperature readings than non-contact optical pyrometers.
Figure 9.7.1: Photograph of a MIFCO Model MT-400 lance pyrometerCopyright © 2013 Copper Development Association Inc. All Rights Reserved.