print this page
AAA

Environment

Loading

Copper-Rotor Motors + Variable Frequency Drives Maximize Savings at a Brass Mill

Download PDF Version [885 Kb]

The Rome, New York, plant of Revere Copper Products, IncThe Rome, New York, plant of Revere Copper Products, Inc., was selected as one of two industrial sites in which to evaluate the cost-effectiveness of copper-rotor motors as replacements for older, less-efficient models.

Photo courtesy of Revere Copper Products

This summary describes the results of a copper-rotor motor evaluation program undertaken by the New York State Energy Research and Development Authority (NYSERDA) at the Rome, New York, brass mill of Revere Copper Products, Inc. A companion summary report describes another portion of that program conducted at the Menands, New York, water treatment plant of the Albany County Sewage District.

NYSERDA initiated the program in 2006 to quantify the economics of replacing old but fully serviceable motors with ultra-high efficiency copper-rotor motors (CRMs). The authority utilizes data of this sort for a program that provides incentives to motor users. In addition, the evaluation program measured operating temperatures of several motors under known loading conditions.

The Copper Development Association (CDA) administered the contract and hired Advanced Energy Corporation, a Raleigh, North Carolina-based certified laboratory, to conduct the analyses at both sites. The full reports are available from NYSERDA or CDA.1

Experimental Plan

Siemens 10-hp induction motorA Siemens 10-hp induction motor of the type used in the evaluation program described here. The motors incorporate a die-cast copper rotor with other design modifications to reduce losses, thereby increasing efficiency by as much as several percentage points above those of average NEMA Premium® motors of comparable sizes.

Photo courtesy of Siemens AG
Ten motors rated between 7.5 hp and 20 hp were evaluated and replaced at the Revere mill, where nine of the motors drove pumps and one, a blower. The motors had been installed between 1967 and 1992. Nameplate efficiencies ranged from 85.5% to 89.5%, which would be expected for pre-EPAct, standard-efficiency models of the time.

Measurements were taken on the old motors’ kW consumption, current, voltage, power factor, time-load profiles and operating temperatures, along with flow rate or pressure (in hydraulic applications). The same data were taken on new motors. Measurements were taken at one-minute intervals over a 2½-hour period. Ambient and motor operating temperatures were measured by Mohawk Valley Predictive Technologies using an infrared technique.

Following reference data collection, old motors were sent to Advanced Energy’s laboratory for physical characterization, including efficiency testing to IEEE Standard 112, Method B, and determination of energy-load profiles. This action was taken because the old motors had been rewound one or more times, and nameplate data were unreliable. Energy-load profiles for the copper-rotor motors were provided by the manufacturer (Siemens).

Back to Top

Gains … and Some Losses

Average nameplate efficiency of six of the ten existing motors for which numbers were available was 86.63%. Advanced Energy found the average measured full-load efficiency to be 86.24% and that the operational efficiency was 86.69%.2 The extensive data analyzed by Advance Energy are omitted here to save space, but are in the report to NYSERDA. The full-load efficiency data are consistent with the small decrease one would expect for rewound motors of this age. Operating efficiencies are slightly higher than full-load nameplate expectations since operation occurred nearer the peak in the power curve.

Dataplate efficiencies of replacement copper-rotor motors ranged from 91.7% at 7.5 hp to 93.6% at 20 hp, averaging 92.42%. The average measured full-load efficiency of the new motors was a nearly identical 92.45%. (CDA has previously reported3 that Siemens rates its copper-rotor motors conservatively.) However, the average calculated operational efficiency of the CRMs was only 89.08%, because four of the motors were being operated at or less than 12% of full rated load, which is far from the optimum utilization.

Despite those clearly oversized motors, the average operational efficiency of the new CRMs was almost 2.4 percentage points higher than that of the motors they replaced. Nevertheless, of the 10 motors installed at Revere, one-half yielded negative savings (losses) compared with the old motors when calculated for a utility rate of $0.14/kWh.

Back to Top

Influence of Centrifugal Loads

All motors selected for evaluation drove centrifugal loads, generally pumps or blowers. In such cases, shaft power is proportional to the cube of rotational speed — the so-called cube rule. CRMs operate with lower slip and, therefore, higher speed than conventional motors. That caused them to draw more power, which offset the gains made by the CRMs’ higher efficiencies. In extreme cases, the results were energy losses.

Centrifugal loads, such as fans, can be slowed with inexpensive pulleys; whereas, pumps are more effectively controlled by slowing the CRMs with variable frequency drives (VFDs). The drives negate the slip/speed penalty and the resultant losses in economic benefits. The NYSERDA program took this effect into account and included in its evaluation additional measurements on motors equipped with a VFD.

Projected savings using VFDs with CRMs were calculated for four motor-pump combinations in which loading conditions between old and new motors were similar. Calculations showed that these four CRMs would generate positive annual cost savings. It was realized after the fact that six of the applications in the motor replacement program had large load variations over time, making comparison of power consumption between old and new motors meaningless.  

Back to Top

Payback and Long-term Savings

A two-year payback is generally acceptable. In addition, in view of the longer service lives expected for CRMs, the projected 10-year savings derived from an investment in high-efficiency CRMs (with VFDs) can be significant. The project examined these savings, including replacing an old motor with other improved types, including NEMA Premium® and EPAct motors.4 The results listed below assume $0.14/kWh, the peak rate paid by Albany County in 2008, and $0.09242/kWh, the average rate paid when the study began in 2006. The rate paid at Revere was not known.

The first three examples in the Revere plant yield payback times between 30 and 37 months at $0.14 per kWh, but the 10-year cost savings amount to several thousand dollars in each case. The cost of the VFD doubles payback times over those for the cost of the new motor alone. CRMs Nos. 2 and 3 (see table below) drive water pumps and No. 6 is a filter media vacuum pump, all directly coupled. For pumps, there is no simpler and cheaper way to reduce the speed by a few percent than a VFD.

Motor No. 9 drives a blower. Here, an inexpensive modification to the pulley and belt drive system may well suffice. Assuming the cost of this modification is negligible, pay-back periods are still rather long, and the 10-year cost saving is slightly negative for the lower of the two electricity rates used here.

Energy savings and payback periods were calculated using MotorMaster+, versions 3.0 and 4.00.06 for EPAct and NEMA Premium motors, respectively.

Centrifugal loads must be examined carefully. Correcting for the higher speed of the CRM with a VFD significantly increases energy savings but requires a larger up-front capital expenditure. For large motors with high duty cycles, the CRM leads to larger 10-year energy savings than replacement with either an EPAct or NEMA Premium motor. For motors with low duty cycles driving centrifugal loads, the CRM + VFD combination does not appear to be cost effective at the utility rates considered here.

Calculated Energy and Cost Savings and Payback Periods for Replacement of Old Motors with Copper-rotor Motors + Variable Frequency Drives
Motor Replacement Cost Motor + VFD ($) Ann. Energy Savings (kWh) Ann. Energy Cost Savings ($) Electricity Rate ($/kWh) Payback Period (Yrs / Mos) 10 year Cost Saving ($)
No. 2
15 hp, 1800 rpm
936.00 + 953.35 5,339 747.46 0.14 2.5 / 30.3 5,585
493.43 0.09242 3.8 / 45.9 3,055
No. 3
15 hp, 1800 rpm
936.00 + 953.35 4,305 602.60 0.14 3.1 / 37.6 4,137
397.87 0.09242 4.7 / 57 2,089
No. 6
15 hp, 3600 rpm
952.25 + 953.35 5,345 748.30  0.14  2.54 / 30.5 5,577
493.98 0.09242 3.86 / 46.3 3,034
No. 9
10 hp, 3600 rpm
693 + 0 702 98.28 0.14 7.06 289
64.88 0.09242 10.7 - 45
Source: Advanced Energy Corporation and Copper Development Association.

Back to Top

Lower Operating Temperatures

The new CRMs operate significantly cooler than the old motors, which is important because heat degrades winding insulation and thereby shortens motor life. An accepted rule of thumb states that a 10°C increase in operating temperature reduces a motor’s life by half.  Bearing life is also adversely effected.  

Temperature measurements were taken in both plants, while the new CRMs and old motors were operating at what, at the time, were thought to be identical loads. Identical temperature guns were used for the measurements. Revere, in addition, employed infrared imaging through a third party vendor, results of which are shown below.

Back to Top

Conclusion

The NYSERDA evaluation program clearly demonstrates the value of replacing old, less-efficient motors with higher-than-NEMA Premium copper-rotor motors, and that replacing EPAct–era or even NEMA Premium motors can also be recommended under certain circumstances. Replacements should be considered in terms of both payback periods as well as long-term savings, since individual situations may influence the results differently. The program also underscores the need to consider concurrent installation of a VFD when centrifugal loads are anticipated. These devices add to initial cost but can provide substantial savings over time. Finally, the NYSERDA program confirms the cooler operating temperatures expected in the more efficient copper-rotor motors, which suggests that they should enjoy longer service lives.

Infrared and Digital Images of Existing Motor No. 2 (top) and New Copper-rotor Motor No. 2 (bottom).
Ambient Max Temp. (AR01) Max Temp. (AR02) Rises (Above Ambient)
22.1°C 71.5°C 66.7°C 49.4°C/44.6°C
Infared Image: I1117-01 Digital Image: 5820
infared photo of motor motor
Ambient Max Temp. (AR01) Max Temp. (AR02) Rises (Above Ambient)
22.1°C 71.5°C 66.7°C 49.4°C/44.6°C
Infared Image: I1117-01 Digital Image: 5820
infared photo of motor motor
Source: Mohawk Valley Predictive Technologies

Back to Top

Footnotes

  1. The New York State Energy Research and Development Authority, In-Plant Demonstration of Electrical Energy Savings Realizable with the Copper-Rotor Motor, Contract No. 10241, Joseph, C. Borowiec, NYSERDA Project Manager, Prepared by Dale T. Peters, Copper Development Association Inc., August 2009.
  2. For calculation methods, see Reference 1 and Agamloh, Emmanuel B., The Partial-Load Efficiency of Induction Motors, IEEE Trans. on Industrial Applications, Vol. 45, No. 1, January/February 2009.
  3. Copper Motor Rotor Update, Copper Development Association, November 2006.
  4. The Energy Independence and Security Act of 2007 raises mandated motor efficiency standards from those of EPAct 2002 to NEMA Premium levels effective in December 2010. Data for EPAct motors in the table assume such motors are available from inventory.
This publication has been prepared solely as resource material for the use of individuals involved in the specification, design, selection and installation of electrical systems. It has been compiled from information provided by one or more of the parties mentioned herein and other information sources Copper Development Association Inc. (CDA) and/or the relevant parties believe to be competent. However, recognizing that each system must be designed and installed to meet the particular circumstances, CDA and the parties mentioned in this publication assume no responsibility or liability of any kind including direct or indirect damages in connection with this publication or its use by any person or organization, AND MAKE NO REPRESENTATIONS OR WARRANTIES OF ANY KIND RELATED TO ITS USE, ACCURACY, COMPLETENESS, UTILITY, AVAILABILITY OR DOCUMENTATION.