print this page

Machined Products

Loading

Free-Cutting Brass for Lower Screw Machine Product Cost: Actuating Sleeve / Air Brake Hose Fitting

ACTUATING SLEEVE

APPLICATION Pneumatic Power
SPECIAL FEATURES High Turnings Ratio, Deep Hole
PART WEIGHT 0.083 lb. (Brass)
BRASS RAW MATERIAL PREMIUM 17% (Including Turnings Allowance)
CYCLE TIME (BRASS) 4.75 sec (606 pieces per hour @ 80% Efficiency)
CYCLE TIME (STEEL) 8.4 sec (300 pieces per hour @ 70% Efficiency)
PRODUCTIVITY GAIN USING BRASS 102%
NET COST SAVINGS (BRASS VS. STEEL) 23% = $58.76 per 1000
NET COST SAVINGS (BRASS VS. PLATED STEEL) 26% = $71.05 per 1000

PRODUCTIVITY AND PLATING SAVINGS SWITCH PART FROM STEEL TO BRASS

This actuating sleeve must be strong and corrosion resistant to work in industrial environments; it's a fairly typical screw machine product. The sleeve is now made from Free-Cutting Brass, Copper Alloy 360, (UNS C36000); it used to be made from 12L14 leaded steel, but it costs about 26% less in brass than it does in steel.

Many designers think that because brass costs more than steel, machined brass parts must cost more too. That's not true for typical screw machine jobs. Only brass rod's off-the-shelf material cost is significantly higher; this actuating sleeve produces more than four times as much turnings weight as it does product and after discounting for the turnings' high value, the net material cost difference is only 17%.

HIGH MACHINABILITY MEANS LOWER PRODUCTION COSTS

When you buy machine parts you are paying for machine time. The faster the cut, the lower the cost, and free cutting brass machines faster than leaded steel. The productivity gained by switching from steel to brass for this actuating sleeve was a very significant 102%. How much can you save on your next screw machine part?

ELIMINATE PLATING COSTS

Steel rusts, brass tarnishes; an important difference. Exposed steel screw machine parts have to be zinc/ chromate plated. Brass parts are ready to use without protective platings. The savings are between 11 and 16 cents per pound of product. If your part has deep holes, threads, or sharp corners, it can be difficult to insure uniform plating on all surfaces. Make the part in brass in you eliminate that concern. The natural corrosion resistance of brass uniformly protects the entire surface. If decorative plating is desired, brass plates more easily and is better looking than plated steel.

BRASS HAS GOOD MECHANICAL PROPERTIES

The strength of half-hard Free-Cutting Brass is in the same range as 12L14 steel. Published nominal values for these materials are:

MATERIAL TENSILE PROPERTIES
YIELD STRENGTH ULTIMATE STRENGTH
C36000 45 ksi 58 ksi
Hot Rolled 12L14 34 ksi 57 ksi
Cold Drawn 12L14 60 ksi 78 ksi

The tensile strength of half-hard brass rod, the most common temper, is about 75% that of cold finished 12L14 steel. Therefore, even if your design is based on the strength of steel, it may be possible to specify brass with no loss of performance and a considerable cost savings.

AIR BRAKE HOSE FITTING

APPLICATION Automotive/Truck
SPECIAL FEATURES Meets DOT Safety Requirements
PART WEIGHT 0.091 lb. (Brass)
BRASS RAW MATERIAL PREMIUM 36% (Including Turnings Allowance)
CYCLE TIME (BRASS) 5.6 sec (515 pieces per hour @ 80% Efficiency)
CYCLE TIME (STEEL) 9.1 sec (277 pieces per hour @ 70% Efficiency)
PRODUCTIVITY GAIN USING BRASS 86%
NET COST SAVINGS (BRASS VS. BARE STEEL) 19% = $46.00 per 1000
NET COST SAVINGS (BRASS VS.PLATED STEEL)* 23% = $59.47 per 1000

STRENGTH PLUS CORROSION RESISTANCE EQUALS SAFETY

This air brake hose fitting, a typical screw machine part, has to be strong and corrosion resistant to meet DOT (Department of Transportation) safety requirements. Originally made from 12L14 leaded steel and zinc/chromate plated to retard corrosion from water and road salts, the fitting is now produced in Free-Cutting Brass, Copper Alloy 360 (UNS C36000). It's just as strong as steel, it doesn't have to be plated . . . and it costs 23% less.

The strength of half-hard Free-Cutting Brass is in the same range as 12L14 steel. Published nominal values for these materials are:

TENSILE PROPERTIES
MATERIAL YIELD STRENGTH ULTIMATE STRENGTH
C36000 45 ksi 58 ksi
Hot Rolled 12L14 34 ksi 57 ksi
Cold Drawn 12L14 60 ksi 78 ksi

The tensile strength of half-hard brass rod, the most common temper, is about 75% that of cold finished 12L14 steel. Therefore, even if your design is based on the strength of steel, it may be possible to specify brass with no loss of performance and a considerable cost savings.

BRASS PARTS COST LESS THAN STEEL

Many designers think that because brass costs more than steel, machined brass parts must cost more too. That's not true for typical screw machine jobs. Only brass rod's off-the-shelf material cost is significantly higher; this air brake hose fitting produces more than three times as much turnings weight as it does product and after discounting for the turnings' high value, the net material cost difference is only 36%.

HIGH MACHINABILITY MEANS LOWER PRODUCTION COSTS

When you buy machine parts you are paying for machine time. The faster the cut, the lower the cost, and free cutting brass machines faster than leaded steel. The productivity gained by switching from steel to brass for this actuating sleeve was a very significant 86%. How much can you save on your next screw machine part?

ELIMINATE PLATING COSTS

Steel rusts, brass tarnishes; an important difference. Exposed steel screw machine parts have to be zinc/ chromate plated. Brass parts are ready to use without protective platings. The savings are between 11 and 16 cents per pound of product. If your part has deep holes, threads, or sharp corners, it can be difficult to insure uniform plating on all surfaces. Make the part in brass in you eliminate that concern. The natural corrosion resistance of brass uniformly protects the entire surface. If decorative plating is desired, brass plates more easily and is better looking than plated steel.

Application Data Sheets

Free-Cutting Brass for Lower Screw Machine Product Cost is available in printable Adobe® Acrobat PDFs * (Click below to download)

Actuating Sleeve

Air Brake Hose Fitting

Cellular Antenna

Fitting Body

HVAC Heating Element Housing

Hydraulic Fitting

Knob Insert

Molded Plastic

Pneumatic Hose Fitting

Temperature Sensor

* For a free download of Adobe® Acrobat Reader please click on the icon below