Free-Cutting Brass for Lower Screw Machine Product Cost: Cellular Antenna / Fitting Body

CELLULAR ANTENNA BASE

APPLICATION Automotive Electronics
SPECIAL FEATURES High Turnings Ratio
PART WEIGHT 0.029 lb. (Brass)
BRASS RAW MATERIAL PREMIUM 14% (Including Turnings Allowance)
CYCLE TIME (BRASS) 3.7 sec (847 pieces per hour @ 80% Efficiency)
CYCLE TIME (LEADED STEEL) 7.1 sec (355 pieces per hour @ 70% Efficiency)
PRODUCTIVITY GAIN USING BRASS 138%
NET COST SAVINGS (BRASS VS. BARE STEEL) 30% = $84.20 per 1000
NET COST SAVINGS (BRASS VS.PLATED STEEL)* 44% = $150.20 per 1000

BRASS COSTS LESS THAN STEEL

This antenna base must be strong and corrosion resistant to work in the exterior environment that surrounds an automobile. It is made from Free-Cutting Brass, Copper Alloy 360, (UNS C36000), and costs about 44% less in brass than it would in 12L14 steel.

Many designers think that because brass costs more than steel, machined brass parts must cost more too. That's not true for typical screw machine jobs. Only brass rod's off-the-shelf material cost is significantly higher. This part produces more than four times as much turnings weight as it does product, and after discounting for the turnings' high value, the net material savings is 14%.

HIGH MACHINABILITY MEANS LOWER PRODUCTION COSTS

When you buy machine parts you are paying for machine time. The faster the cut, the lower the cost, and free cutting brass machines faster than leaded steel. The productivity gain by switching from steel to brass for this part is an impressive 138%.

BRASS HAS GOOD MECHANICAL PROPERTIES

The strength of half-hard Free-Cutting Brass is in the same range as 12L14 steel. Published nominal values for these materials are:

MATERIAL TENSILE PROPERTIES
YIELD STRENGTH ULTIMATE STRENGTH
C36000 45 ksi 58 ksi
Hot Rolled 12L14 34 ksi 57 ksi
Cold Drawn 12L14 60 ksi 78 ksi

The tensile strength of half-hard bras rod, the most common temper, is about 75% that of cold finished 12L14 steel. ELIMINATE PLATING COSTS Steel rusts, brass tarnishes; an important difference. Exposed steel parts have to be zinc/ chromate plated. Brass parts are ready to use without protective platings. The savings are between 11 and 16 cents per pound of product. If your part has deep holes, threads, or sharp corners, it can be difficult to insure uniform plating on all surfaces. Make the part in brass in you eliminate that concern. The natural corrosion resistance of brass uniformly protects the entire surface.

FITTING BODY

APPLICATION Underwater Pump Assembly
SPECIAL FEATURES Teflon Coated
PART WEIGHT 0.11 lb (Brass)
BRASS RAW MATERIAL PREMIUM 23% (Including Turnings Allowance)
CYCLE TIME (BRASS) 4.5 sec (641 pieces per hour @ 80% Efficiency)
CYCLE TIME (LEADED STEEL) 8.0 sec (315 pieces per hour @ 70% Efficiency)
PRODUCTIVITY GAIN USING BRASS 102%
NET COST SAVINGS (BRASS VS. BARE STEEL) 22%, $35.17 per 1000
NET COST SAVINGS (BRASS VS.PLATED STEEL)* 3% = $6.87 per 1000

A CASE OF REVERSE ENGINEERING

Sometimes materials selection decisions can be changed long after a part has been in production. That's the case with this fitting body, which forms part of an underwater pump assembly. It was made for many years using tellurium-treated leaded steel because its design required high machinability. One alert screw machine shop recognized that still higher machinability, and maybe some cost reductions, could be gained by switching from steel to Free-Cutting Brass, Copper Alloy 360 (UNS C36000). The screw machine shop brought a test run to the customer, the customer recognized the quality of the product, changed the specs to brass and gave the enterprising machine shop the order. Today, many hundreds of thousands of parts later, the fitting is still being made from brass.

Brass can be cost-competitive with steel because its machinability is so much higher than steel's-about five times higher, in fact. And brass turnings are worth a lot of money; when recycled, they greatly reduce brass's net cost to the customer.

BRASS STRENGTH EQUIVALENT

Like most screw machine products, this pump part operates at stresses well within the limits of both brass and steel. In fact, brass and steel are often interchangeable because their strengths overlap the same range.

MATERIAL TENSILE PROPERTIES
YIELD STRENGTH ULTIMATE STRENGTH
C36000 45 ksi 58 ksi
Hot Rolled 12L14 34 ksi 57 ksi
Cold Drawn 12L14 60 ksi 78 ksi

One more thing: this fitting body must be Teflon-coated, whether it's made from steel or brass. This presents no problem, as brass readily accepts most commercial coatings and finishes, TefIon included.

Application Data Sheets

Free-Cutting Brass for Lower Screw Machine Product Cost is available in printable Adobe® Acrobat PDFs * (Click below to download)

Actuating Sleeve

Air Brake Hose Fitting

Cellular Antenna

Fitting Body

HVAC Heating Element Housing

Hydraulic Fitting

Knob Insert

Molded Plastic

Pneumatic Hose Fitting

Temperature Sensor

* For a free download of Adobe® Acrobat Reader please click on the icon below