Dimensions and Physical Characteristics of Copper Tube: Medical Gas, K and L
| Nominal or Standard Size, inches | Nominal dimensions, inches | Calculated values (based on nominal dimensions) | ||||||
|---|---|---|---|---|---|---|---|---|
| Outside diameter | Inside diameter | Wall thickness | Cross sectional area of bore, sq. inches | Internal surface, sq. ft. per linear ft. | Weight of Tube only, pounds per linear ft. | Contents of tube, cu. ft. per linear ft | ||
| 1/4 | K | .375 | .305 | .035 | .073 | .0789 | .145 | .00051 |
| L | .375 | .315 | .030 | .078 | .0825 | .126 | .00054 | |
| 3/8 | K | .500 | .402 | .049 | .127 | .105 | .269 | .00088 |
| L | .500 | .430 | .035 | .145 | .113 | .198 | .00101 | |
| 1/2 | K | .625 | .527 | .049 | .218 | .130 | .344 | .00151 |
| L | .625 | .545 | .040 | .233 | .143 | .285 | .00162 | |
| 5/8 | K | .750 | .652 | .049 | .334 | .171 | .418 | .00232 |
| L | .750 | .666 | .042 | .348 | .174 | .362 | .00242 | |
| 3/4 | K | .875 | .745 | .065 | .436 | .195 | .641 | .00303 |
| L | .875 | .785 | .045 | .484 | .206 | .455 | .00336 | |
| 1 | K | 1.125 | .995 | .065 | .778 | .261 | .839 | .00540 |
| L | 1.125 | 1.025 | .050 | .825 | .268 | .655 | .00573 | |
| 1-1/4 | K | 1.375 | 1.245 | .065 | 1.222 | .326 | 1.04 | .00845 |
| L | 1.375 | 1.265 | .055 | 1.26 | .331 | .884 | .00873 | |
| 1-1/2 | K | 1.625 | 1.481 | .072 | 1.72 | .388 | 1.36 | .0120 |
| L | 1.625 | 1.505 | .060 | 1.78 | .394 | 1.14 | .0124 | |
| 2 | K | 2.125 | 1.959 | .083 | 3.01 | .522 | 2.06 | .0209 |
| L | 2.125 | 1.985 | .070 | 3.09 | .520 | 1.75 | .0215 | |
| 2-1/2 | K | 2.625 | 2.435 | .095 | 4.66 | .638 | 2.93 | .0323 |
| L | 2.625 | 2.465 | .080 | 4.77 | .645 | 2.48 | .0331 | |
| 3 | K | 3.125 | 2.907 | .109 | 6.64 | .761 | 4.00 | .0461 |
| L | 3.125 | 2.945 | .090 | 6.81 | .761 | 3.33 | .0473 | |
| 3-1/2 | K | 3.625 | 3.385 | .120 | 9.00 | .886 | 5.12 | .0625 |
| L | 3.625 | 3.425 | .100 | 9.21 | .897 | 4.29 | .0640 | |
| 4 | K | 4.125 | 3.857 | .134 | 11.7 | 1.01 | 6.51 | .0811 |
| L | 4.125 | 3.905 | .110 | 12.0 | 1.02 | 5.38 | .0832 | |
| 5 | K | 5.125 | 4.805 | .160 | 18.1 | 1.26 | 9.67 | .126 |
| L | 5.125 | 4.875 | .125 | 18.7 | 1.28 | 7.61 | .130 | |
| 6 | K | 6.125 | 5.741 | .192 | 25.9 | 1.50 | 13.9 | .180 |
| L | 6.125 | 5.854 | .140 | 26.8 | 1.53 | 10.2 | .186 | |
| 8 | K | 8.125 | 7.583 | .271 | 45.2 | 1.99 | 25.9 | .314 |
| L | 8.125 | 7.725 | .200 | 46.9 | 2.02 | 19.3 | .325 | |