Dimensions and Physical Characteristics of Copper Tube: ACR (Air-Conditioning and Refrigeration Field Service)
| Nominal or Standard Size, inches | Nominal dimensions, inches | Calculated values (based on nominal dimensions) | |||||||
|---|---|---|---|---|---|---|---|---|---|
| Outside diameter | Inside diameter | Wall thickness | Cross sectional area of bore, sq. inches | External surface, sq. ft. per linear ft. | Internal surface, sq. ft. per linear ft. | Weight of Tube only, pounds per linear ft. | Contents of tube, cu. ft. per linear ft. | ||
| 1/8 | A | .125 | .065 | .030 | .00332 | .0327 | .0170 | .0347 | .00002 |
| 3/16 | A | .187 | .128 | .030 | .0129 | .0492 | .0335 | .0575 | .00009 |
| 1/4 | A | .250 | .190 | .030 | .0284 | .0655 | .0497 | .0804 | .00020 |
| 5/16 | A | .312 | .248 | .032 | .0483 | .0817 | .0649 | .109 | .00034 |
| 3/8 | A | .375 | .311 | .032 | .076 | .0982 | .0814 | .134 | .00053 |
| D | .375 | .315 | .030 | .078 | .0982 | .0821 | .126 | .00054 | |
| 1/2 | A | .500 | .436 | .032 | .149 | .131 | .114 | .182 | .00103 |
| D | .500 | .430 | .035 | .145 | .131 | .113 | .198 | .00101 | |
| 5/8 | A | .625 | .555 | .035 | .242 | .164 | .145 | .251 | .00168 |
| D | .625 | .545 | .040 | .233 | .164 | .143 | .285 | .00162 | |
| 3/4 | A | .750 | .680 | .035 | .363 | .196 | .178 | .305 | .00252 |
| A | .750 | .666 | .042 | .348 | .196 | .174 | .362 | .00242 | |
| D | .750 | .666 | .042 | .348 | .196 | .174 | .362 | .00242 | |
| 7/8 | A | .875 | .785 | .045 | .484 | .229 | .206 | .455 | .00336 |
| D | .875 | .785 | .045 | .484 | .229 | .206 | .455 | .00336 | |
| 1-1/8 | A | 1.125 | 1.025 | .050 | .825 | .294 | .268 | .655 | .00573 |
| D | 1.125 | 1.025 | .050 | .825 | .294 | .268 | .655 | .00573 | |
| 1-3/8 | A | 1.375 | 1.265 | .055 | 1.26 | .360 | .331 | .884 | .00875 |
| D | 1.375 | 1.265 | .055 | 1.26 | .360 | .331 | .884 | .00875 | |
| 1-5/8 | A | 1.625 | 1.505 | .060 | 1.78 | .425 | .394 | 1.14 | .0124 |
| D | 1.625 | 1.505 | .060 | 1.78 | .425 | .394 | 1.14 | .0124 | |
| 2-1/8 | D | 2.125 | 1.985 | .070 | 3.09 | .556 | .520 | 1.75 | .0215 |
| 2-5/8 | D | 2.625 | 2.465 | .080 | 4.77 | .687 | .645 | 2.48 | .0331 |
| 3-1/8 | D | 3.125 | 2.945 | .090 | 6.81 | .818 | .771 | 3.33 | .0473 |
| 3-5/8 | D | 3.625 | 3.425 | .100 | 9.21 | .949 | .897 | 4.29 | .0640 |
| 4-1/8 | D | 4.125 | 3.905 | .110 | 12.0 | 1.08 | 1.02 | 5.38 | .0833 |
| A = Annealed Temper, D = Drawn Temper | |||||||||