Bending Guide for Copper Tube

Nominal Standard Size, in Tube Type Temper Minimum Bend, Radius*, in
1/4 K,L Annealed 3/4
3/8 K,L Annealed 1-1/2
K,L,M Drawn 1-3/4
1/2 K,L Annealed 2-1/4
K,L,M Drawn 2-1/2
3/4 K,L Annealed 3
K,L Drawn 3
1 K,L Annealed 4
1-1/4 K,L Annealed 9
NOTE: * The radii stated are the minimums for mechanical bending equipment only.