Melting Temperature Ranges for Copper and Copper Alloys, Brazing Filler Metals, Brazing Flux and Solders

7A.
7B.
 
* Melting ranges of solder alloys are in accordance with the alloy manufacturers product information and may not match the melting ranges shown in ASTM B32.