Commodity Tube

Copper Tube - Types, Standards, Applications, Tempers, and Lengths
Tube type Color code Standard Application¹ Commercially available lengths²
Nominal or standard sizes Drawn Annealed
Type K Green ASTM B 88³ - Domestic water service and distribution
- Fire protection
- Solar
- Fuel/fuel oil
- HVAC
- Snow melting
Straight lengths:
1/4 inch to 8 inch 20 ft. 20 ft.
10 inch 18 ft. 18 ft.
12 inch 12 ft. 12 ft.
Coils:
1/4 inch to 1 inch 60 ft.
100 ft.
1 1/4 inch and
1 1/2 inch
60 ft.
2 inch 40 ft.
45 ft.
Type L Blue ASTM B 88 - Domestic water service and   distribution
- Fire protection
- Solar
- Fuel/fuel oil
- Natural Gas
- Liquefied petroleum (LP) gas
- HVAC
- Snow melting
Straight lengths:
1/4 inch to 8 inch 20 ft. 20 ft.
12 inch 18 ft. 18 ft.
Coils:
1/4 to 1 inch 60 ft.
100 ft.
1 ¼ inch to 1 ½ inch 60 ft.
2 inch 40 ft.
45 ft.
Type M Red ASTM B 88 - Domestic water service and distribution
- Fire protection
- Solar
- Fuel/fuel oil
- HVAC
- Snow melting
Straight lengths:
¼ inch to 12 inch 20 ft. N/A
DWV Yellow ASTM B 306 - Drain, waste, vent
- Solar
- HVAC
Straight lengths:
1 ¼ inch to 8 inch 20 ft. N/A
ACR Blue ASTM B 280 - Air conditioning
- Refrigeration
- Natural gas
- Liquefied petroleum (LP) gas
Straight lengths:
3/8 inch to 4 1/8 inch 20 ft. 4
Coils:
1/8 inch 1 5/8 inch 50
OXY, MED
OXY/MED
OXY/ACR
ACR/MED
(K) Green
(L) Blue
ASTM B 819 - Medical gas Straight lengths:
¼ inch to 8 inch 20 ft. N/A
1. There are many other copper and copper alloy tubes and pipes available for specialized applications. For information on these products, contact the Copper Development Association, Inc.
2. Individual manufacturers may have commercially available lengths in addition to those shown in this table.
3. Tube made to other ASTM standards is also intended for plumbing applications, although ASTM B 88 is by far the most widely used. ASTM Standard Classifications B 698 lists six plumbing tube standards including B 88.
4. Available as special order only.
Back to top

DIY Video Podcasts

Video screenshot Soldering Preparation

View More Videos

Building & Architecture News

Building and Architecture News thumbnail

October '11: The Fall issue focuses on the benefits of copper at healthcare institutions. Read about a new copper HVAC system that makes AC systems more energy efficient; a medical campus that relies on copper for their state-of-the-art information network; copper trends in building and construction projects; how copper provides shielding for MRI systems to improve accuracy, and the importance of copper to ensure cleanliness, reliability and efficiency in medical gas systems.

Read More News

Highlights

Learn about copper's 50-year warranty program

50-year warranty seal

CDA Tube, Pipe and Fittings Council members:


Industry News: Selection of recent copper tube, pipe and fittings industry developments, technology advances, etc to keep you up to date.


The entire Copper Tube Handbook can be downloaded in pdf format [6 Mb].

The Copper Tube Handbook