Ceridian Corporate Headquarters
Bloomington, MN
New Construction
Architect
Hammel, Green and Abrahamson, Inc.Minneapolis, MN
Copper System: Laminated copper facing on a thermoplastic core on a stainless steel subgirt system
For this curtain wall system a composite copper panel was used. This panel offers strength and a dead flat surface preventing "oil canning". Oil canning is a term used to describe the waviness that is common with sheet metal roof and wall systems.