print this page

Architecture

Loading

Gutters and Downspouts:
Introduction

The design of gutter and downspout assemblies is an area of building design which demands special attention. Leaking gutters and downspouts can cause serious damage to a building's interior as well as exterior, and repairs can be expensive.

Maintenance, durability and longevity are important factors to consider when designing gutters and downspouts. Copper is an intelligent choice of materials because of its low maintenance, high resistance to corrosion and long life. Even in severe climates such as marine atmospheres, a well designed copper gutter and downspout assembly will provide many years of low maintenance service.

Other metals used in gutter and downspout assemblies require frequent repainting or recoating to maintain their durability. Copper is an inherently corrosion resistant material which does not require special coatings to maintain its durability or its appearance.

The ease with which a material can be joined to form a continuous, leak-free water conductor is also important. Copper's inherent properties make it an easy material to form and solder. Thus, strong leakproof joints are readily achievable with copper.

Design Principles for Roof Drainage Systems

The building type, its appearance and location have a direct influence on the design of the roof drainage system. They determine the roof area, slope and rainfall intensity. They also influence the use of gutters and downspouts, roof drains and scuppers.

The process of calculating the required size of gutters and downspouts involves:

  1. Obtaining rainfall intensity for the building location.
  2. Determining the spacing and locations of downspouts.
  3. Calculating design roof areas.
  4. Sizing the downspouts.
  5. Sizing the gutters.

Rainfall Intensity

Rainfall intensity is measured over a 5-minute period. It is recorded, in inches per hour, as the resulting accumulation as if the intensity remained constant for a full hour. Table 4.4.2 shows the rainfall intensity for major U.S. cities. The table is divided into two sections, A and B. These sections represent the intensities which are likely to be exceeded once in 10 years, and once in 100 years, respectively.

The table also shows the calculated roof area which can be drained per square inch of downspout. It is based on the assumption that during a rainfall with an intensity of 1 inch per hour, each square inch of downspout can drain 1200 square feet of roof. If the intensity is doubled the downspout capacity is halved, or 600 sq. ft.; if it is tripled the capacity is one third, and so on.

Table 4.4.2 - Rainfall Data and Drainage Factors
AREA A
Storms which should be exceeded only once in 10 years
B
Storms which should be exceeded only once in 100 years
1
5 Minute intensity (in/hr)
2
Area drained per sq. inch of downspout (sq. ft.)
1
5 Minute intensity (in/hr)
2
Area drained per sq. inch of downspout (sq. ft.)
Alabama Birmingham 7.5 160 10.1 120
  Mobile 8.2 150 10.8 110
Alaska Fairbanks 2.1 570 3.8 320
  Juneau 1.7 710 2.3 520
Arizona Phoenix 5.6 210 8.8 140
  Tucson 6.1 200 19.1 130
Arkansas Bentonville 7.4 160 10.2 120
  Little Rock 7.4 160 10.0 120
California Los Angeles 4.9 240 6.7 180
  Sacramento 2.5 480 3.9 310
  San Diego 2.2 550 3.1 390
  San Francisco 2.7 440 3.7 320
Colorado Denver 5.7 210 9.1 130
  Boulder 6.4 190 9.4 130
Connecticut Hartford 6.2 190 8.7 140
District of Columbia   7.1 170 9.7 120
Florida Jacksonville 7.9 150 10.1 120
  Miami 7.7 160 9.8 120
  Tampa 8.3 140 10.8 110
Georgia Atlanta 7.3 160 9.9 120
Hawaii Honolulu 8.7 140 12.0 100
  Kahului 7.0 170 12.0 100
  Hilo 17.4 70 19.2 60
  Lihue 10.4 120 14.4 80
Idaho Boise 1.8 670 3.3 360
Illinois Chicago 6.8 180 9.3 130
Indiana Indianapolis 6.8 180 9.4 130
Iowa Des Moines 7.3 160 10.3 120
Kansas Wichita 7.5 160 10.5 110
Kentucky Louisville 6.9 170 9.4 130
Louisiana New Orleans 8.3 140 10.9 110
Maine Portland 5.4 220 7.6 160
Maryland Baltimore 7.1 170 9.7 120
Massachusetts Boston 5.3 230 7.2 170
Michigan Detroit 6.4 190 8.9 130
Minnesota Minneapolis 7.0 170 10.0 120
Missouri Kansas City 7.4 160 14.4 80
  St. Louis 7.1 170 9.9 120
Montana Helena 1.8 670 3.1 390
  Missoula 1.8 670 2.4 500
Nebraska Omaha 7.4 160 10.5 110
Nevada Reno 2.3 520 4.5 270
  Las Vegas 2.1 570 5.2 230
New Jersey Trenton 6.7 180 9.3 130
New Mexico Albuquerque 4.0 300 6.7 180
  Santa Fe 4.5 270 6.4 190
New York Albany 6.5 180 9.1 130
  Buffalo 6.0 200 8.4 140
  New York City 6.7 180 9.2 130
North Carolina Raleigh 7.3 160 9.8 120
North Dakota Bismarck 6.6 180 9.8 120
Ohio Cincinnati 6.8 180 9.3 130
  Cleveland 6.3 190 8.8 140
Oklahoma Oklahoma City 7.6 160 10.5 110
Oregon Baker 2.2 550 3.8 320
  Portland 2.1 570 3.0 400
Pennsylvania Philadelphia 6.8 180 9.4 130
  Pittsburgh 6.4 190 8.8 140
Rhode Island Providence 5.6 210 7.8 150
South Carolina Charleston 7.2 170 9.4 130
Tennessee Memphis 7.4 160 10.0 120
  Knoxville 6.7 180 9.0 130
Texas Fort Worth 7.6 160 10.5 110
  Dallas 7.6 160 10.5 110
  Houston 8.2 150 10.8 110
  San Antonio 7.6 160 10.5 110
Utah Provo 3.0 400 5.2 230
  Salt Lake City 2.8 430 4.3 280
Virginia Norfolk 7.1 170 9.5 130
Washington Seattle 2.1 570 3.3 360
  Spokane 2.1 570 3.5 340
West Virginia Parkersburg 6.6 180 9.1 130
Wisconsin Madison 6.8 180 9.5 130
  Milwaukee 6.6 180 9.1 130
Wyoming Cheyenne 5.7 210 9.9 120

Downspout Locations

The locations of down-spouts depends on the configuration, architectural features and appearance of the building. The technical considerations include:

  1. Each downspout should drain a maximum of 50 feet of gutter. Gutter expansion characteristics may further limit the distances, since water cannot flow past an expansion joint.
  2. Avoid locations where water must flow around a corner to reach a downspout.
  3. In locations where icing occurs, downspouts on the north side of the building should be avoided, if possible.

Expansion Joint Spacing

Expansion joints in copper gutters must be provided to allow for the natural expansion and contraction of copper caused by thermal changes. In general, long straight runs should have joints spaced a maximum of 48 feet apart. Expansion joints may also be required at changes in gutter width or depth, at corners and at end conditions. Based upon the desired joint spacing, designers should consult Table 4.4.3 to determine the required gauge of copper gutter, width of gutter bottom and angle of gutter sides.

Design Area for Pitched Roofs

The roof area to be drained is a key factor in designing gutters and downspouts. The area of roof contributing runoff to each gutter and downspout should be determined. The maximum accumulation of rainfall occurs when it falls perpendicular to the roof plane. With flat roofs, it is a simple matter of calculating area, since the true roof area is equal to plan area.

When a roof is pitched, its plan area is less than its true area. However, using the true area in the calculations has typically resulted in oversized gutters, downspouts and drains. Table 4.4.1 shows the factors that should be used to determine the design area for pitched roofs. The plan roof area should be multiplied by this factor. The result is the design roof area that is used to calculate the required sizes of downspouts.

Table 4.4.1 - Area Factor for Pitched Roofs
Pitch, in/ft Area Factor
Level to 3 1.00
4 to 5 1.05
6 to 8 1.10
9 to 11 1.20
12 1.30

Downspout Sizing

Downspouts should have a cross-sectional area of at least 7 square inches, except for small areas such as porches and canopies. Their size should be constant throughout their length.

The design roof area is divided by the area of roof shown in Table 4.4.2, column A2 or B2 (see discussion above), to give the minimum required area for each downspout. See Table 4.4.10.1 for standard downspout sizes.

Gutter Sizing

The minimum required size of a gutter is related to the intensity of rainfall and the area of roof that drains into the gutter. The latter depends on the length of the gutter, which is related to locations of downspouts, expansion joints, and gutter ends.

Other factors considered in the design of gutters, include the size and spacing of outlets, the shape of the gutter, and the pitch of the roof. The gutter size must be capable of handling even fast moving water from a steep roof.

Table 4.4.4 is used to determine the required width and depth of a gutter. To do this, a ratio, M which equals the depth divided by the width, is initially assumed. Starting with the length of the gutter, L, follow a vertical line until the ratio, M, is reached. At this point follow a horizontal line to the left until the vertical line of rainfall intensity x design area, IA, is crossed. The required gutter width can be read from the diagonal lines. If the intersection lies between two lines, use the higher value. Finally, the width is multiplied by the ratio, M, to determine the depth.

The size of gutters with an irregular shape can be determined by calculating the required size of a rectangular gutter which closely matches in profile and cross-sectional area, the irregularly shaped gutter.

Table 4.4.5 shows an example of the complete process.

Design Handbook

Available in 2 formats:

Web Version
and
Desktop Application

Download AutoCAD Files

AutoCAD Detail Files
[ZIP - 4.5MB] is a complete set of CAD files for the designs shown in Architectural Details.

The AutoCAD files for individual details can be downloaded from individual topic pages by clicking the CAD File button next to an individual detail.

Order Design Handbook

Available in CDA's Publications
(publication #A4050).