A Copper Alliance Member
Tube, Pipe & Fittings
- Overview
- Key Copper Benefits
- TechCorner
- Designing and Installing Copper Piping Systems
- Is There A Problem With Embedding Copper Tube In Concrete?
- Why Do I Have Blue/Green Staining Of My Bathroom Fixtures
- Corrosion of Mixed Metal Fire Sprinkler Systems
- Is It True That Electrolysis Can Cause My Copper Tube To Fail?
- Glossary of Technical Terms
- How to Prevent Corrosion of Copper Tube in Underground or Buried Applications
- Can Copper Tube Be Used in Steam and Steam Condensate Piping Systems?
- Soldering and Brazing Explained
- Project Managers
- DIY: Do It Proper With Copper Video Series
- Applications
- Resources & Tools
- Installing Copper Piping Systems
- Technical References
- HVAC/R
- Copper DX Geothermal Heat Pumps
TechCorner
The TechCorner has been developed by the Copper Development Association to provide industry professionals with a targeted selection of white papers and answers to technical questions of interest to plumbers, installers, contractors and engineers. A glossary of technical terms that defines the meanings of specific terminology used in this section is also provided here.
Topics List
Soldering and Brazing Explained
For many years the two most common methods of joining copper tube and fittings have been soldering and brazing. These tried and true methods are in a number of ways similar, yet there are also several distinct differences that set them apart. This paper explains the similarities and highlights the differences between the two joining processes to help determine which joining method is most desirable...<more>
Can Copper Tube Be Used in Steam and Steam Condensate Piping Systems?
Everyone knows that copper tube has a proven history in use in a variety of applications, however a common question is "can I use copper tube in a steam system?" Just like in water systems, copper tube has long been used in both steam and steam condensate piping systems. The key to its successful use in either high- or low-pressure steam systems is in choosing the appropriate joining method for the service....<more>
How to Prevent Corrosion of Copper Tube in Underground or Buried Applications
Out-of-sight, out-of-mind. That's the phrase that comes to mind for all who have installed copper and copper alloy piping systems in buried, underground applications. An expectation well supported by the excellent corrosion resistance of copper alloys used in these applications. An expectation that may not be realized when this out-of-site, out-of-mind philosophy extends to the practices used in installing the system.<more>
Is It True That Electrolysis Can Cause My Copper Tube To Fail?
Electrolysis is an overused and misused term when applied to copper tube. True electrolysis, or electrolytic corrosion, as it is more properly designated with regard to piping, is caused by an imposed (external) stray DC current and virtually ceased to occur with the disappearance of the trolley-car that was powered by high amperage DC current... Usually, what people are really referring to when they say electrolysis is galvanic or dissimilar metal corrosion...<more>
Corrosion of Mixed Metal Fire Sprinkler Systems
This paper is in response to the many questions that are asked regarding automatic fire sprinkler systems using copper tube and fittings in conjunction with conventional steel pipe. The capability of mixed metals specifically to resist galvanic corrosion, is sometimes questioned. The concern expressed focuses primarily on composite systems where copper tube branch lines and cross mains are used in connection with steel pipe feed mains, risers and standpipes....<more>
Why Do I Have Blue/Green Staining Of My Bathroom Fixtures?
Green or blue water staining are names given to a general corrosive attack that on rare occasions occurs in buildings that have been plumbed in copper. In most instances this phenomenon manifests itself shortly after a new plumbing system is put into continuous service and then eventually goes away. Notice of this situation occurs, and concern generally arises, when it causes a slight blue or green discoloration in the water or, more commonly on surfaces that come in contact with the water such as plumbing fixtures. There are a number of processes that can cause this discoloration and staining, two of them much more common than the others...<more>
Is There A Problem With Embedding Copper Tube In Concrete?
It is completely acceptable to bury/embed both hard drawn and annealed copper water tube in concrete. Decades of satisfactory service experience with the use of copper tube for in-floor radiant heating systems, water distribution systems and snow melting systems attest to the compatibility of copper tube embedded, encased or in contact with concrete. It is also acceptable to run a copper water tube through a concrete floor or wall, provided that allowance is made for the lateral thermal expansion and movement of the tube and protection of the tube from abrasion...<more>
What Is Most Important When Designing And Installing Copper Piping Systems?
Copper tube and fittings have a remarkable track record for plumbing use. The ancient Egyptians are known to have used copper pipes for transporting water and, in modern times, copper tube has been used for over 75 years for plumbing in the U.S. It's a fact that the majority of problems with a copper piping installation can be prevented by proper design and installation practices. It's also true that a major cause of difficulty is erosion corrosion, a mechanically induced failure, which may be caused by number of conditions ...<more>
Please check back regularly as we will be adding new items to this section on a regular basis.
DIY Video Podcasts
Building & Architecture News
October '11: The Fall issue focuses on the benefits of copper at healthcare institutions. Read about a new copper HVAC system that makes AC systems more energy efficient; a medical campus that relies on copper for their state-of-the-art information network; copper trends in building and construction projects; how copper provides shielding for MRI systems to improve accuracy, and the importance of copper to ensure cleanliness, reliability and efficiency in medical gas systems.
Highlights
Learn about copper's 50-year warranty program
CDA Tube, Pipe and Fittings Council members:
Industry News: Selection of recent copper tube, pipe and fittings industry developments, technology advances, etc to keep you up to date.
The entire Copper Tube Handbook can be downloaded in pdf format [6 Mb].